Impact value of Sa106 Gr B

113 views
Skip to first unread message

Manish Kumar

unread,
May 7, 2024, 7:56:32 AM5/7/24
to material...@googlegroups.com
Hi,
Please share the impact value of carbon steel SA 106 Gr B.


Regards
Manish Kumar 

venkateswara reddy Desireddy

unread,
May 7, 2024, 10:55:53 AM5/7/24
to material...@googlegroups.com
Sa106 gr B not a impact tested material. It's not recommended for low temperature service. Refer ASME Sec VIII div1 UCS 66 for impact values.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHfQ4k6n2KTYcBFpAXdGOfh_4zF_a%3DggpuXXhecaP-Bmju0Tuw%40mail.gmail.com.

Amol Betkar

unread,
May 8, 2024, 2:49:08 AM5/8/24
to material...@googlegroups.com

Dear,

The impact value of carbon steel SA 106 Gr B, often expressed as Charpy V-notch (CVN) impact test values, can vary depending on factors such as the specific heat treatment, testing temperature, and sample orientation. However, a common minimum requirement for SA 106 Gr B is an average absorbed energy value of 20 ft-lb (27 J) at room temperature.

This value indicates the amount of energy absorbed by the material during fracture in the Charpy V-notch impact test. It's an important measure of the material's toughness and its ability to withstand sudden loading or impact.

For precise impact values, it's advisable to refer to the material's specific requirements as outlined in relevant standards or specifications, as they may vary slightly depending on the source or application.

Regards,

AB


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHfQ4k6n2KTYcBFpAXdGOfh_4zF_a%3DggpuXXhecaP-Bmju0Tuw%40mail.gmail.com.


--
Best regards,

Amol K.B
B.E(Mech), CSWIP 3.2.2, NACE CIP 1 & ASNT LII(4M)