Porosity Problem in Monel 400 Electrode ENiCu7

80 views
Skip to first unread message

PSS

unread,
Jun 14, 2024, 6:58:51 AM6/14/24
to Materials & Welding
Please provide the solution for Porosity problem in N04400 during SMAW welding with electrode of ENiCu7.

Thanks in advance.

pravin.n...@gmail.com

unread,
Jul 5, 2024, 6:29:00 AM7/5/24
to Materials & Welding
For such issue Electrodes with low hydrogen content ENiCu-7 are typically recommended for welding nickel copper alloys like Monel.
Hope you have taken care basic things of baking of electrode, Cleanliness, Welding parameters.

Regards,
Pravin Nimbalkar