A234 WPB & WPBW

2,415 views
Skip to first unread message

Zameer Mohammed

unread,
May 8, 2008, 4:27:31 AM5/8/08
to material...@googlegroups.com

Dear Friends,

 

As per our specification,

 

36'' EQ TEE & 36'' x 24'' RED TEE is C.S. A234 GR WPB BW.

 

The vendor is offering - C.S. A234 GR. WPBW, BW

 

How can I convince my client that WPBW will confirm to the Chemical Requirement, Tensile Requirement, for WPB.

 

Thank you,

 

Regards,

 

 

Sabir

 

                                               

Nick

unread,
May 9, 2008, 2:53:01 AM5/9/08
to Materials & Welding
Dear Sabir,
Please refer page No.385 of Sec II Part - A (A234).

WPBW is mandatory Marking on the fittings. So the requirements are met
as per A234.

If there is still problem please reply to this.

Rushabh C. Kapadia

On May 8, 1:27 pm, "Zameer Mohammed" <dreamthinkw...@gmail.com> wrote:
> Dear Friends,
>
> As per our specification,
>
> 36'' EQ TEE & 36'' x 24'' RED TEE is C.S. A234 GR WPB BW.
>
> The vendor is offering - C.S. A234 *GR. WPBW*, BW
>
> How can I convince my client that *WPBW *will confirm to the Chemical

Zameer Mohammed

unread,
May 12, 2008, 11:01:10 AM5/12/08
to material...@googlegroups.com

Dear Mr. Rushabh,

 

I understand that in SA 234, for WPB there are two method of construction.

Seamless - WPB

Welded - WPBW

 

Is it possible to get Fittings above 16'' as Seamless Construction?

 

I have to procure a 36'' EQUAL TEE and 36'' x 24'' RED TEE. All the vendors are offering Welded Construction, but the Client prefers Seamless. Am I right at the statement that, all fittings above 16'' are Welded Construction only.

 

AM I RIGHT…..?

 

Kindly advice me…

 