ASME full form of SA - A 387/A 387M – 06a

2,759 views
Skip to first unread message

Akhilesh singh

unread,
Oct 17, 2014, 2:40:41 AM10/17/14
to material...@googlegroups.com
Plz help me regarding such full-form:

1. ASME full form of SA - A 387/A 387M – 06a ............. what does means of "SA" - "A" 387 ................. "A387M" - "06a"..........................???

                          or
             A 387/A 387M – 06a

2. Grade P91 steel (A 387/A 387M – 06a)
    what does me "P"  & "91"

Harish Kannepalli

unread,
Oct 17, 2014, 4:18:01 AM10/17/14
to material...@googlegroups.com
American Society of Mechanical Engineers Section A, Developed by ASTM Commitee A01.11 A387/A387M is adopted from ASTM A387/387M where M stands for Metric; as Americans follow inch-pound system; 06 is year of publication, a-is first revision in that year
P91-P is desgination; 9%-Chromium, 1%Molybdenum

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.



--
Regards,
Mr. Harish.

Mohit Aggarwal

unread,
Oct 17, 2014, 4:18:05 AM10/17/14
to materials-welding

SA means Specification for analysis of ferrous material and 387 is specification in which specific material grade class falls and P.is the no given by ASME to specific group.of material...

Best Regards,
Mohit Aggarwal.

--

Anup N K E

unread,
Oct 17, 2014, 6:22:09 AM10/17/14
to material...@googlegroups.com

P91 stands for grade of the material , where P stands for pipe, 91 stands for 9% Cr, 1% Mo and Vanadium . P  no. Of grade P91 material is 15E.

Grade P9 has composition 9% Cr - 1% Mo whose P no. Is 5B.

Regards,
Anup N K E

Binoy Lonappan

unread,
Oct 21, 2014, 5:38:07 AM10/21/14
to materials-welding

“SA” is not an acronym.  It is just a designation given to the ferrous material specifications adopted by ASME to distinguish it from material specifications from other organizations.  There are also ASME “SB” specifications and they are for the nonferrous material specifications.  

 

The ASME SA- specifications are in ASME Section II, Part A and the ASME SB- specifications are in ASME Section II, Part B.  The latest edition is the 2013 edition.

With Regards
Binoy Lonappan

QAC Engineer





Adeel Rafique

unread,
Nov 18, 2014, 12:58:40 PM11/18/14
to material...@googlegroups.com
SA is an ASME specification for the analysis of ferrous materials. A387 / A387M are the specification number for that particular material. 06a is the year when it was approved by ASME. While 'P" is the number assigned to that material because of its properties. the numerical figure 91 attributes the composition of elements it contains. I found the regarding info in www.weldpedia.com

Annamalai Ram

unread,
Aug 8, 2023, 11:37:03 PM8/8/23
to Materials & Welding
SA: "S" stands for ASME material specification, adopted from ASTM. 
"A" stands for Ferrous material SA 387/M387M, is Pressure Vessel Plates, Cr-Mo Alloy Steel, SA 387 is in US conventional units(FPS), "SA 387M" is metric version, 06a is 2006 edition addanda.