Reg: Welding Procedure Qualification as per ISO15614

78 views
Skip to first unread message

s.harikrish s

unread,
Sep 23, 2024, 6:05:01 AM9/23/24
to Materials & Welding
Dear experts... I have one clarification in ISO15614; I have a WPS qualified in Group No. 6.1 with Group No. 5.1... Shall I use this WPS for Group No. 6.1 with Group No. 5.2. As per table 5 in ISO 15614 we can use it. But I have a concern I have to use filler material with different chemical and Mechanical property (Cl.8.4.4) like instead of ER80S-B2 I will use ER90S-B3. My Qualification level as per ISO15614 is Level II. Pls suggest your opinion with back up. Thanks in advance...

Kannayeram Gnanapandithan

unread,
Sep 24, 2024, 1:22:41 AM9/24/24
to material...@googlegroups.com
As per Table 5, Foot note b , it may not qualify

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015, ISO 3834, EN 15085, 
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Mon, Sep 23, 2024 at 3:34 PM s.harikrish s <harikr...@gmail.com> wrote:
Dear experts... I have one clarification in ISO15614; I have a WPS qualified in Group No. 6.1 with Group No. 5.1... Shall I use this WPS for Group No. 6.1 with Group No. 5.2. As per table 5 in ISO 15614 we can use it. But I have a concern I have to use filler material with different chemical and Mechanical property (Cl.8.4.4) like instead of ER80S-B2 I will use ER90S-B3. My Qualification level as per ISO15614 is Level II. Pls suggest your opinion with back up. Thanks in advance...

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/06653aef-d841-4470-8830-a011ad28cb2fn%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages