Do we need to run new PQR for using TIG dressing/wash to correct pipe alignment.

27 views
Skip to first unread message

solomon

unread,
Aug 13, 2015, 1:15:24 AM8/13/15
to Materials & Welding
Dear All Expert
Refer to QW 404.14 of ASME Sec IX.
Do we need to run new PQR for using TIG dressing/wash to correct pipe alignment as per ASME B31.3& Sec IX.
In my opinion I think process of TIG dressing should not be subjected to QW 404.14 because it's doesn't join two part together.
I'd appreciate all of your sharing and reference.

Regards
Reply all
Reply to author
Forward
0 new messages