size of welding specimen

31 views
Skip to first unread message

Souravbohray

unread,
Jun 15, 2018, 11:34:00 PM6/15/18
to Materials & Welding
is there any standard size of weld specimen for single vee groove weld according to asme sec 9

Bharat Kumar

unread,
Jun 16, 2018, 7:07:37 AM6/16/18
to material...@googlegroups.com
I think it's 150x300 for one plate so sums up to 300x300

On Sat 16 Jun, 2018, 9:03 AM Souravbohray, <ermechsou...@gmail.com> wrote:
is there any standard size of weld specimen for single vee groove weld according to asme sec 9

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Er Sourav Bohray

unread,
Jun 16, 2018, 8:00:45 AM6/16/18
to material...@googlegroups.com
ya u are right but my AI wants proof in written in asme code.. i look out asme sec 9 but i that only given take size in which size for tension bend sufficent

On 16 Jun 2018 4:37 p.m., "Bharat Kumar" <asopa....@gmail.com> wrote:
I think it's 150x300 for one plate so sums up to 300x300

On Sat 16 Jun, 2018, 9:03 AM Souravbohray, <ermechsou...@gmail.com> wrote:
is there any standard size of weld specimen for single vee groove weld according to asme sec 9

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

--
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/b8Yx0olyqI4/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.

Nithin Joseph

unread,
Jun 17, 2018, 1:50:06 AM6/17/18
to material...@googlegroups.com
Hi,

There is no requirement of size of specimen in code. However it should selected based on the testing requirements. Like for carrying out tensile test, width of min 300mm is required including weld, width wise. Length will depend on kind of testing required such as hardness, impact etc. AI cannot question this as it is the sole responsibility of manufacturer. 
Regards,
Dsilva

Er Sourav Bohray

unread,
Jun 17, 2018, 1:55:19 AM6/17/18
to material...@googlegroups.com
thanks a lot 300 width for tensile and 150 for bend

123 456

unread,
Jun 29, 2018, 3:15:38 AM6/29/18
to material...@googlegroups.com
Either refer ASME BPVC Section-IX mechanical test related pages or contact an established material testing laboratory engaged in this business. AI has no role in test specimen size selection. Manufacturer or Contractor is responsible for everything till final date of product guarantee period . 

On Fri, Jun 15, 2018 at 9:29 PM, Souravbohray <ermechsou...@gmail.com> wrote:
is there any standard size of weld specimen for single vee groove weld according to asme sec 9