JIS SS 41 MATERIAL

3,862 views
Skip to first unread message

KASHKOUSHA

unread,
Feb 2, 2015, 4:39:38 AM2/2/15
to Materials-welding
Dear all
kindly, what is the equivalent of the material JIS SS 41& the suitable filler metal for welding
Thanks for your cooperation
Regards

Hesham
 
H.KASHKOUSHA

LALU RAJENDRAN

unread,
Feb 3, 2015, 3:50:31 AM2/3/15
to material...@googlegroups.com
Dear Hesham,

JIS 3101 SS400 (SS 41) is equivalent to ASTM A36 in mechanical properties except elongation. You can use ER70S-X and E70XX for Welding. See the below link for further details.



Regards,
LALU
LINKS MIDDLE EAST

Thanks & Regards,

LALU R.P

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/330449626.799446.1422868999662.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

Reply all
Reply to author
Forward
0 new messages