When is supplementary essential variable becomes Essential ?

95 views
Skip to first unread message

PK M

unread,
Jul 18, 2021, 10:50:21 PM7/18/21
to material...@googlegroups.com
Dears,

When does the supplementary essential variable become Essential ? 

thanks

Manivannan p

unread,
Jul 19, 2021, 12:11:59 AM7/19/21
to material...@googlegroups.com
Supplementary Essential variable is to be considered and addressed in PQR/WPS when the WPS is qualified with CHARPY IMPACT test and whenever the material requires IMPACT TEST per code/standard.
Thanks,
MANIVANNAN.P

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFoQ_nfYY8%3D0_GwfXjVnFFbjQU%3Dc-z1ugVsNjKzVpsvF-yS5JQ%40mail.gmail.com.

Vishwas Keskar

unread,
Jul 19, 2021, 12:12:05 AM7/19/21
to material...@googlegroups.com
When Notch Toughness requirements are specified, then supplementary essential variables become  Essential variable. 
Regards

--