My dept was having one PQR qualified as per AWS D1.1 with double V Groove weld.
When we try to qulify our welders for a specific project,where in the requirement is for single v groove weld.
We have Conducted the test with 16mm plate (Single V preparation)
The third party qualified the welders.Is this ok
 
Because as per AWS D 1.1 groove configuration is an essential variable
 
Is any one clarify this
 
Regards
R.Venkataraman  


Need more space to upload pictures? Get 25 GB online storage with Windows Live SkyDrive! Try it!

Akshay Kumar takes on the two reigning Bollywood Khans. Catch the action on MSN Entertainment! Check it out!

Muhammed Ibrahim

unread,
Feb 25, 2009, 4:30:08 AM2/25/09
to material...@googlegroups.com
Dear Venkit raman,
 
Groove design is essential variable only for procedure qualification. For welders groove design is not an essential variable( please see Table 4.12 & Table 4.1) in AWS D1.1.
 
Regards,
 
Muhammed Ibrahim

2009/2/25 Radhakrishnan Venkatraman <r_ven...@hotmail.com>

babu k

unread,
Feb 27, 2009, 9:30:12 AM2/27/09
to material...@googlegroups.com
Hi,
 
When u qualify a welder through the WPS, you should follow the WPS grrove design as per D1.1(See 4.18.3) ;
 
otherwise follow the configuration given in D1.1  ;
 
Thanks;
 
K.Babu
 
Welding Engineer
 