The material specification for the casting is ASTM A148/A148M Type IV Steel, Grade 150-135. However, the casting is being produced using AISI 8630 alloy. We are currently looking for a suitable weld wire that meets the ASTM A148 Grade 150-135 specification. Please do let me know you recommendation or suitable wire which can meet the casting strengths.