Re: Impact Test

50 views
Skip to first unread message

prateik tolani

unread,
Feb 19, 2020, 5:09:11 AM2/19/20
to material...@googlegroups.com
Dear experts

We have job with MDMT -30 and -36 Deg C
Shell/Dish - SA516 Gr 70N
material will be received in impact tested condition
need to know whether weld impact test is required or not?
thickness is 8-10 mm.
welding electrode 7018-1

On Wed, Feb 19, 2020 at 2:06 PM prateik tolani <tolani...@gmail.com> wrote:
Dear experts

We have job with MDMT -30 and -36 Deg C
Shell/Dish - SA516 Gr 70N
material will be received in impact tested condition
need to know whether weld impact test is required or not?
thickness is 8-10 mm.
welding electrode 7018-1


Thanks 
prateik

Ramesh

unread,
Feb 19, 2020, 5:50:45 AM2/19/20
to material...@googlegroups.com

I presume there is no specific service requirements based impact testing and plates are normalized


As per Figure UCS-66M of ASME Sec 8 Div.1, The material 516 fouls under curve D. the impact testing is exempted up to -48°C for your thickness. So not required for your case.


Thanks and Regards

Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"



On Wed, Feb 19, 2020 at 3:39 PM prateik tolani <tolani...@gmail.com> wrote:
Dear experts

We have job with MDMT -30 and -36 Deg C
Shell/Dish - SA516 Gr 70N
material will be received in impact tested condition
need to know whether weld impact test is required or not?
thickness is 8-10 mm.
welding electrode 7018-1

On Wed, Feb 19, 2020 at 2:06 PM prateik tolani <tolani...@gmail.com> wrote:
Dear experts

We have job with MDMT -30 and -36 Deg C
Shell/Dish - SA516 Gr 70N
material will be received in impact tested condition
need to know whether weld impact test is required or not?
thickness is 8-10 mm.
welding electrode 7018-1


Thanks 
prateik

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGNY-_AMkqLQr%2BV0KXTtf%3DG%2BX03SpPg8z92ePJqHXO0PJpZctg%40mail.gmail.com.

Ramesh

unread,
Feb 19, 2020, 7:05:25 AM2/19/20
to material...@googlegroups.com

I presume there is no specific service requirements and plates are normalized

 

As per Figure UCS-66M of Sec 8 Div.1, The plate material 516 fouls under curve D. the impact testing is exempted up to -48°C .

 

Reg welding, The electrode E7018-1 is guaranteed impact values at -45°C. Refer Table 3 of SFA 5.1.

 

But its better to have impact tested PQRs for company future use. 

Thanks and Regards

Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"


On Wed, Feb 19, 2020 at 3:39 PM prateik tolani <tolani...@gmail.com> wrote:
Dear experts

We have job with MDMT -30 and -36 Deg C
Shell/Dish - SA516 Gr 70N
material will be received in impact tested condition
need to know whether weld impact test is required or not?
thickness is 8-10 mm.
welding electrode 7018-1

On Wed, Feb 19, 2020 at 2:06 PM prateik tolani <tolani...@gmail.com> wrote:
Dear experts

We have job with MDMT -30 and -36 Deg C
Shell/Dish - SA516 Gr 70N
material will be received in impact tested condition
need to know whether weld impact test is required or not?
thickness is 8-10 mm.
welding electrode 7018-1


Thanks 
prateik

--

Prashant Rane

unread,
Feb 20, 2020, 1:27:56 AM2/20/20
to material...@googlegroups.com
Impact for Weld is not required as E 7018-1 is upto minus 45 deg c, as per Code.  Check the GTAW Filler if you are using any.  

Most important check material of flange and pipe

Regards,
Prashant

On Wed, Feb 19, 2020, 2:09 PM prateik tolani <tolani...@gmail.com> wrote:
Dear experts

We have job with MDMT -30 and -36 Deg C
Shell/Dish - SA516 Gr 70N
material will be received in impact tested condition
need to know whether weld impact test is required or not?
thickness is 8-10 mm.
welding electrode 7018-1

On Wed, Feb 19, 2020 at 2:06 PM prateik tolani <tolani...@gmail.com> wrote:
Dear experts

We have job with MDMT -30 and -36 Deg C
Shell/Dish - SA516 Gr 70N
material will be received in impact tested condition
need to know whether weld impact test is required or not?
thickness is 8-10 mm.
welding electrode 7018-1


Thanks 
prateik

--

Kannayeram Gnanapandithan

unread,
Feb 20, 2020, 1:27:56 AM2/20/20
to materials-welding

LALIT VADADORIYA

unread,
Feb 20, 2020, 1:27:56 AM2/20/20
to material...@googlegroups.com
YES, PQR QUALIFICATION WITH IMPACT TEST IS TO BE CARRIED OUT FOR SAFE SIDE. 
Regards

Lalit Vadadoriya
Dy.Manager(Piping)
Engineers India Limited



On Wed, Feb 19, 2020 at 3:39 PM prateik tolani <tolani...@gmail.com> wrote:
Dear experts

We have job with MDMT -30 and -36 Deg C
Shell/Dish - SA516 Gr 70N
material will be received in impact tested condition
need to know whether weld impact test is required or not?
thickness is 8-10 mm.
welding electrode 7018-1

On Wed, Feb 19, 2020 at 2:06 PM prateik tolani <tolani...@gmail.com> wrote:
Dear experts

We have job with MDMT -30 and -36 Deg C
Shell/Dish - SA516 Gr 70N
material will be received in impact tested condition
need to know whether weld impact test is required or not?
thickness is 8-10 mm.
welding electrode 7018-1


Thanks 
prateik

--

harenath jha

unread,
Feb 20, 2020, 1:27:56 AM2/20/20
to material...@googlegroups.com
As per asme section ix its an supplementry essential variable. Hence required

Ramesh

unread,
Feb 20, 2020, 2:13:22 AM2/20/20
to material...@googlegroups.com
70N - Yes, normalized plates,, Just overlooked ! 

Thanks and Regards


Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"


Ramesh

unread,
Feb 20, 2020, 2:13:30 AM2/20/20
to material...@googlegroups.com
To be precious

Refer  UCS 67- Highlighted line

image.png

Thanks and Regards


Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"