Dear All,

What could be code reference of construction code of heating coils
inside the tank (API 650) especially when we do the pneumatic test of
these coils. the general piping code is ASME 31.3 & 31.4.. Kindly
advise

Thanks in advance
Kumar

joseph mbé

unread,
Jan 31, 2013, 1:15:26 AM1/31/13
to material...@googlegroups.com
Should be ASME B31.1 Power piping codes.

Regards
 
Joseph Faustin Mbe
QA/QC Engineer
TEL CMR (00237) 33129846
TEL CG (00242) 057388009
BP 1155 Pointe Noire
Yesterday is the pass, tomorrow is the future; and today? Today is the present, the gift: Enjoy it!
 


De : Kumar kerala <sk79...@gmail.com>
À : materials-welding <material...@googlegroups.com>
Envoyé le : Mercredi 30 janvier 2013 12h23
Objet : [MW:16645] Heating coils- API 650 tanks
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsub...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsub...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.




Reply all
Reply to author
Forward
0 new messages