Ferrite–Austenite Phase Requirement for DSS as per ASME Sec IX

36 views
Skip to first unread message

Nambirajan Avudaiappan

unread,
Jun 4, 2026, 2:13:57 AM (5 days ago) Jun 4
to material...@googlegroups.com

Dear Experts,

Good morning!

Has anyone performed ferrite–austenite phase evaluation for Duplex Stainless Steel (DSS)?

As per my understanding, this requirement has been incorporated in ASME Section IX under Non-Mandatory Appendix M (M-600). I would appreciate if you could share your experience, procedures followed, or any practical challenges faced during implementation.

Whether we can do with any machines without help of labratories

Looking forward to your valuable inputs.


image.png

atul jha

unread,
Jun 4, 2026, 3:05:53 AM (5 days ago) Jun 4
to material...@googlegroups.com
The steps are :
1. Establish the PQR with extreme care as welding parameters will play crucial role in phase formation.
2. Do the ASTM 562 ( ferrite count by metallography) and ferritoscope( this is a portable machine and to be used on production weld principle is magnetic here ).
3. Welding on production weld shall be done by welding parameters established during PQR establishment.
4. With ferritoscope production weld phase can be measured.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJuyB2W4yRfBs9N1zWWFd6EfNApA8u7-dqMYgr0HsXCkEDJVhA%40mail.gmail.com.

pradip kumar Sil

unread,
Jun 4, 2026, 3:05:54 AM (5 days ago) Jun 4
to material...@googlegroups.com
Hi,
I could not find this requirement in the ASME Section IX (2023 edition). Could you please confirm which edition you are referring to?  

Mandatory Appendix upto K

image.png

--

Nambirajan Avudaiappan

unread,
Jun 4, 2026, 3:10:40 AM (5 days ago) Jun 4
to material...@googlegroups.com

manish kulkarni

unread,
Jun 4, 2026, 3:10:45 AM (5 days ago) Jun 4
to material...@googlegroups.com

Nambirajan Avudaiappan

unread,
Jun 4, 2026, 3:31:15 AM (5 days ago) Jun 4
to material...@googlegroups.com

This requirement is not applicable to PQR; it is applicable to WPQR.

For WPQR, can we measure the ferrite content using a ferritoscope during production in the shop, instead of performing the point count method?


Regards,


Nambirajan A


manish kulkarni

unread,
Jun 4, 2026, 3:40:14 AM (5 days ago) Jun 4
to material...@googlegroups.com
Yes , it should be done in PQR as well . Convince customer for the approach

pradip kumar Sil

unread,
Jun 7, 2026, 12:12:42 AM (yesterday) Jun 7
to material...@googlegroups.com
 Appendix M is a non-mandatory appendix. Accordingly, its requirements cannot be enforced by the Client unless they are expressly stated in the contract or incorporated by reference in an applicable project document.  