Dear Experts,
Can anyone suggest, which standard need to be followed for PWHT chart recorder calibration with use of Simulator.

Regards, 
Darshan

pradip kumar Sil

unread,
Jun 6, 2019, 7:40:44 AM6/6/19
to materials-welding
You will get that information PFI Standard

Temp. recording instrument is 6 month

AWS D10.10 you can check also



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABDq6gj-wuZ5xPg8c%2BgG_LLckLJcHFhRBR0ucHa2CBjjkzwtbw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Reply all
Reply to author
Forward
0 new messages