Clarify UG-81 TOLERANCE FOR FORMED HEADS

1,565 views
Skip to first unread message

anhtrangnghieng

unread,
Jun 2, 2018, 1:05:50 AM6/2/18
to material...@googlegroups.com

Dear Experts, 

Please help me to clarify requirement of  UG-81 TOLERANCE FOR FORMED HEADS , ASME Sec VIII Div 1 2017. 

The inner surface of Ellipsoidal head shall not deviate inside the specified shape by more than 5/8% of ID: This tolerance shall be applied for all Head ( Crown R & Knuckle r) or only for Crown R portion ?

Please also provide the reference. 



Thank in advance.

Gigi




ajay pathak

unread,
Jun 4, 2018, 7:42:59 AM6/4/18
to material...@googlegroups.com
This clause is applied to all head and talking about "Overcrowing" & Under crowning".

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Reply all
Reply to author
Forward
0 new messages