API 650 - 8.1.2.2 The following requirements apply to vertical joints

269 views
Skip to first unread message

Isac Passaura

unread,
Aug 10, 2021, 11:16:23 PM8/10/21
to Materials & Welding
Dear Experts,

I have a doubt about API 650 - 8.1.2.2 a) and b), when it says:
"For butt-welded joints in which the thinner shell plate is less than or equal to 10 mm" 
does this apply to the entire shell? For example in the figure below, do I consider the entire shell in item a)? 

thinner shell plate.png
Many thanks.

Best Regards
Isac Passaura


james gerald

unread,
Aug 11, 2021, 3:39:58 AM8/11/21
to material...@googlegroups.com
The lowest section is of thickness 16mm and shall comply with the requirement of (b) (spot radiography requirements)and the remaining with less than 10mm shell thickness shall follow (a) as per figure below. Considering the lowest shell of 16mm is one course the radiography requirement of intersections shall follow (a)

Inline image


Thanks & Regards

J.Gerald Jayakumar




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d1f97dfc-9abe-418f-89b9-a83af152062cn%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages