Dear Experts,
I have qualified PQR on 10 mm thickness, groove angle 45 Deg,
Thickness range - 3-20 mm
Range for Groove angle is 40-65
PQR on 30 mm thickness, groove angle 50 deg
Thickness range - 15-60 mm
Range of groove angle is 45-70
Can I combine above to PQRs for groove angle range 40-70.
Job thickness is 60 mm.
Groove angle is 40 deg .
Is there any reference in DNVGL-OS-C401 for groove angle range on minimum side.
Your expert advice is awaited.
Regards,
Vishal R Chakote