AWS-D1.1 Procedure qualified in groove

69 views
Skip to first unread message

mithlesh kumar

unread,
Jun 8, 2023, 2:27:00 AM6/8/23
to Materials & Welding
Dear members,

I have an query related to AWS D1.1 Edition 2020 i have qualified PQR in CJP groove weld  may it also qualified for fillet weld ?


Regards
Mithlesh
QA/QC

paresh patel

unread,
Jun 10, 2023, 8:08:12 AM6/10/23
to material...@googlegroups.com
Yes

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/edf657d9-ebe4-46e0-8c82-878f0bc75532n%40googlegroups.com.

Faisal Sattar

unread,
Jun 10, 2023, 8:55:50 AM6/10/23
to material...@googlegroups.com
Any PQR qualified in Butt joint (Groove weld), automatically qualified for all weld joint type and design as per ASME Section 9.

--

Kannayeram Gnanapandithan

unread,
Jun 10, 2023, 9:03:26 AM6/10/23
to materials-welding
for sec 9, joint design is non essential variables.  