High YS to Low YS

43 views
Skip to first unread message

mubeenaws

unread,
Apr 9, 2016, 11:25:16 PM4/9/16
to material...@googlegroups.com

Good day all 
Please help me out by providing u r advise on below request. 

We have a qualified WPS with 75K YS material as per Sec-IX, can we use on material with 65K YS for welding? 

Please provide your feed back with reference clause. 

Thanks and Regards 
Munden


Sent from my Samsung device

meisam shokri arfaei

unread,
Apr 9, 2016, 11:45:03 PM4/9/16
to material...@googlegroups.com
The YS is not a concern by its own.

You have to refer to the reference standard/code and check the material grouping system and essential variables which may cause re-qualification.

Regards

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/rjpr5c1o0br8nc1ww9xs5w5r.1460209404507%40email.android.com.
For more options, visit https://groups.google.com/d/optout.



--
M. Shokri Arfaei
ASNT NDT Level III
International Welding Engineer





Mohit Aggarwal

unread,
Apr 10, 2016, 4:55:50 AM4/10/16
to materials-welding

It depends on Base Material P No and group No given in Sec IX and additional  requirements if any.

Best Regards,
Mohit Aggarwal.

--

Shashank Vagal

unread,
Apr 10, 2016, 4:55:54 AM4/10/16
to material...@googlegroups.com
Dear Meisam,

Considering generally, a  high YS material would be most suited for structural applications if other factors do not interfere adversely.
 
BR,
Shashank C Vagal (Quality Adviser)
Neo Metal-Analyst & NDT Services (Approved by IBR, Thermax, etc)
Regd Office: 301, PRATHAMESH, M G Rd – Mahant Rd, Vile Parle East, Mumbai 400 057 INDIA
Tel : +91 22 2611 6640(+91) 9821386292 /  8082395502 / 9819191861    
Works Office: A-25, Geet Siddhee, Sector No. 11, Pradhikaran, Gat No. 62, Boradewasti, Moshi, Dist: Haveli, PCMC, Pune – 411044, Maharashtra, India
      
www.neometalanalystndt.com / enq...@neometalanalystndt.com / nach...@yahoo.com



From: meisam shokri arfaei <meisam...@gmail.com>
To: material...@googlegroups.com
Sent: Sunday, 10 April 2016 9:12 AM
Subject: Re: [MW:24659] High YS to Low YS

Vivek Pandey

unread,
Apr 10, 2016, 4:56:12 AM4/10/16
to material...@googlegroups.com
dear Munden

please refer trailing para extracted from ASME section IX. I hope this may help you

QW-200.3 To reduce the number of welding procedure
qualifications required, P‐Numbers are assigned to
base metals dependent on characteristics such as composition,
weldability, and mechanical properties, where this
can logically be done; and for steel and steel alloys
(Table QW/QB-422) Group Numbers are assigned additionally
to P‐Numbers. These Group Numbers classify
the metals within P‐Numbers for the purpose of procedure
qualification where notch‐toughness requirements are
specified. The assignments do not imply that base metals
may be indiscriminately substituted for a base metal
which was used in the qualification test without
consideration of the compatibility from the standpoint of
metallurgical properties, postweld heat treatment, design,
mechanical properties, and service requirements. Where
notch toughness is a consideration, it is presupposed that
the base metals meet the specific requirements.


Regards,

Vivek Pandey
QC Engineer