Filler wire

35 views
Skip to first unread message

sujit kumar

unread,
Mar 4, 2025, 1:53:59 AM3/4/25
to material...@googlegroups.com
Dear expert,

What filler wire We should use to weld SB466 C70600  to SB466 C70600 material.

What parameter should we use to weld that material. Specially when it will get crack??


Thanks and regards
Sujit

Vishwas Keskar

unread,
Mar 4, 2025, 7:36:06 AM3/4/25
to material...@googlegroups.com, material...@googlegroups.com
Pl send chemical composition 
Sent from my iPhone

On 4 Mar 2025, at 12:23 PM, sujit kumar <sujitku...@gmail.com> wrote:


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAFonYWPKiRumE8qRDSg0wX1zAUZFCooUUJpKt8E7nQjqFwhPkw%40mail.gmail.com.

Deerendra Karanth

unread,
Mar 4, 2025, 11:55:56 AM3/4/25
to material...@googlegroups.com

As per my understanding, the composition is typically as follows:

Copper (Cu): 88.0 - 90.0%

Nickel (Ni): 9.0 - 11.0%

Iron (Fe): 1.0 - 2.0%

Manganese (Mn): 0.5 - 1.0%

Zinc (Zn): ≤ 1.0%

Lead (Pb): ≤ 0.05%

Sulfur (S): ≤ 0.02%

Carbon (C): ≤ 0.05%

Phosphorus (P): ≤ 0.02%

Could you kindly confirm if this composition aligns with the latest specifications for SB466 C70600, or provide any additional insights regarding permissible variations?

BR, 

Deerendra. 


sridhar cn

unread,
Mar 4, 2025, 12:26:19 PM3/4/25
to material...@googlegroups.com
As Chemistry of SB466 C70600 (Copper-Nickel alloy, CuNi10Fe1Mn) is
Cu- 88 to 90%
Ni-  9 to 11%
Fe- 1 to 1.8%
Mn- up to 1%
to weld  SB466 C70600 to itself, the recommended filler wire is ERCuNi (Copper-Nickel). This filler metal matches 
the composition of the base material and ensures good corrosion resistance, particularly in marine environments. 
ERCuNi is specifically designed for welding 90/10 and 70/30 Copper-Nickel alloys and provides excellent mechanical 
properties and compatibility with the base material.
Argon or Argon+Helium (for deeper penetration) could be used for shielding.

Sridhar.
------------------------------------------------------------------------------------------------------------------------------

--

Vishwas Keskar

unread,
Mar 4, 2025, 10:24:03 PM3/4/25
to material...@googlegroups.com, material...@googlegroups.com
Use
ERCuNi wire or
ERNiCu-7

Sent from my iPhone

On 4 Mar 2025, at 10:56 PM, sridhar cn <sridha...@gmail.com> wrote: