Dear Pinaki,
The Material comparison form is your client standard format / requirements. Which at this stage may not be fulfilled completely, what ever details as required in your client format for compliances shall have been addressed during the procurement of the plates.
Also, your client requirements as given in the form are non-mandatory or supplementary as per the particular material specification (A537-2013) and A20.
Hence, you may ask waiver from your client on these requirements and the it shall not be any problem for AI to accept the plate material.
Regards,
PARAG PANSARE
Mob number +601115656517
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOt02TCyda1PRG2iFj-FORe%3DZaD0Y_Qzah80semHyWxcnM6fQQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Mr Boxi,
Advise NISCO to replace all the MTCs as per ASME material specifaction.
As a Contractor / Buyer you would have commented on the draft MTC before printing as a final copy. You would have atleast specified on PR and PO.
Now only the option to replace the MTC, Client will not accept the deviations. Hence, disciss with NISCO for the new MTC as per ASME Section II.
Regards
P Govindan
L&T HCI-PQM,
Abu Dhabi.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOt02TDS-zADEKZan7x-NcDia7rSr%3Dety9FTOk134vCpxYksFw%40mail.gmail.com.