Dear Expert,

For Austenitic stainless steel ( Type 304L, 316L) whats acceptance criteria for ASTM A 262 - Practice C as a recomanded practice.

Standard says it should be defined by user how ever client specification is silent in my case.

Thank you

james gerald

unread,
Jun 2, 2023, 5:15:32 AM6/2/23
to material...@googlegroups.com
General acceptance standard for Material selection as below.

Inline image


Thanks & Regards

J.Gerald Jayakumar




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOdsS43jqObAzFfbmdTLSfEGXikYSJJ1O3E74F822dwV20TKjA%40mail.gmail.com.

Adnan Ziad

unread,
Jun 2, 2023, 5:15:35 AM6/2/23
to material...@googlegroups.com
In our project we follow practice E 
Standard: ASTM A262 Practice E
(Acceptance criteria: No fissures or cracking at 20X magnification)