welding consumables PMI

131 views
Skip to first unread message

ms viswanathan

unread,
Feb 22, 2016, 2:20:04 AM2/22/16
to material...@googlegroups.com
Dear Experts,
Please advise how to check welding filler wire for PMI check.is there any procedure or standards.
Regards, MSV

c sridhar

unread,
Feb 22, 2016, 4:54:00 AM2/22/16
to material...@googlegroups.com
Filler material chemistry will have variation with welded chemistry.

SS filler meal will have additional Cr & Ni to compensate evaporation losses 
during welding. Hence welding to be carried out using particular filler metal 
and it's chemistry to be analysed as per code. 

You have to follow ASME sec. II part C and respective classification. For example 
SS filler wire comes under SFA 5.9. GMAW filler metal specified under SFA. 5.18 
and like wise.
 
C Sridhar.
Technical Adviser - Welding,
for Alsta Pristine Engineering Private Limited,. Bangalore

( SS, AL fabricators & A venture of Advance Eng. Training & Inspection Services). Chennai,

Mobile nos: 0 94449 71097, 0 7406 326326, .


Please don't print this e-mail unless you really need to. Save the environment.


Life is like bicycling. To move on, keep balancing  throughout.. 


 



From: 'ms viswanathan' via Materials & Welding <material...@googlegroups.com>
To: material...@googlegroups.com
Sent: Monday, 22 February 2016 11:20 AM
Subject: [MW:24348] welding consumables PMI

Dear Experts,
          Please advise how to check welding filler wire for PMI check.is there any procedure or standards.
Regards, MSV

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsub...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1991395429.648011.1456120201562.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.


Reply all
Reply to author
Forward
0 new messages