Using A350/LF2 instead of A105

615 views
Skip to first unread message

Ezat Adel

unread,
Dec 21, 2013, 1:44:43 AM12/21/13
to materials-welding
is there a limitation to use A350/LF2 instead of A105 forged material, there is no low temp. condition the working temp. assumed to be max. 200 C and the impact test is not required.
also as i know A350/LF2 can used from -46C to 345C nd A105 can used from -29C to 427C is this information is documented and if please advice.



G Pad

unread,
Dec 22, 2013, 2:24:22 AM12/22/13
to material...@googlegroups.com
Ezat adel
You can use ASTM A350 Gr LF2 instead of A 105 provided max design temperature is 200 Deg C.

G Padmanabhan


On Sat, Dec 21, 2013 at 12:14 PM, Ezat Adel <ezatad...@gmail.com> wrote:
is there a limitation to use A350/LF2 instead of A105 forged material, there is no low temp. condition the working temp. assumed to be max. 200 C and the impact test is not required.
also as i know A350/LF2 can used from -46C to 345C nd A105 can used from -29C to 427C is this information is documented and if please advice.



--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.



--
Nothing is difficult, you just didn´t understand it yet...
 
With Warm regards,

G.Padmanabhan
+96895685853

aada

unread,
Dec 23, 2013, 2:26:23 PM12/23/13
to material...@googlegroups.com

Please, could yo send us Design Conditions? Pressure and Temperature?

 

 

 

ATENTAMENTE
Antonio Alonso Diaz Arriaga
044 5559952007

De: material...@googlegroups.com [material...@googlegroups.com] en nombre de Ezat Adel [ezatad...@gmail.com]
Enviado: sábado, 21 de diciembre de 2013 12:44 a.m.
Para: materials-welding
Asunto: [MW:19666] Using A350/LF2 instead of A105

is there a limitation to use A350/LF2 instead of A105 forged material, there is no low temp. condition the working temp. assumed to be max. 200 C and the impact test is not required.
also as i know A350/LF2 can used from -46C to 345C nd A105 can used from -29C to 427C is this information is documented and if please advice.