SET PRESSURE FOR PRESSURE RELIEF VALVE FOR HYDROTESTING OF POWER PIPING

3,149 views
Skip to first unread message

shailesh dave

unread,
Jan 30, 2008, 3:40:22 AM1/30/08
to material...@googlegroups.com
Dear Mr Dave
Could you please resend this query with proper subject line? And also in future please don’t hit reply button while starting new thread, instead u can create new mail and send to
 
Best regards
Raghuram Bathula

From: shailesh dave [mailto:snd...@yahoo.com]
Sent: Wednesday, January 30, 2008 1:46 PM
To: material...@googlegroups.com
Subject: Re: [MW:537] Re: 533] Filler metal for P 11 (O/L SS 347) to P8
 
Dear Members,
 
Can anybody tell me at what pressure of hydrotest be safety relief valve set. What is the reference code.
 
Regards,
 
S.N.Dave
 
QA/QC Manager
 


Never miss a thing. Make Yahoo your homepage.

Raghuram Bathula

unread,
Jan 30, 2008, 10:52:06 AM1/30/08
to Materials & Welding
When conditions require that a pressure test will be maintained for a
period of time during which the testing medium in the system would be
subject to thermal expansion, provision should be made for relief of
excess pressure.

I have no idea about any code requirement but normal practice as per
my experience for Valve Setting Pressure is Test pressure plus
lesser of 10 psi (0.69 Bar a) or 7% of the test pressure



> From: shailesh dave [mailto:snd2...@yahoo.com]
> Sent: Wednesday, January 30, 2008 1:46 PM
> To: material...@googlegroups.com
> Subject: Re: [MW:537] Re: 533] Filler metal for P 11 (O/L SS 347) to P8
>
> Dear Members,
>
> Can anybody tell me at what pressure of hydrotest be safety relief valve set. What is the reference code.
>
> Regards,
>
> S.N.Dave
>
> QA/QC Manager
>
> ---------------------------------

shailesh dave

unread,
Jan 30, 2008, 11:13:59 AM1/30/08
to material...@googlegroups.com
DEAR Mr. RAGHURAM,
 
THANKS FOR THE REPLY.
 
REGARDS,
 
S.N.DAVE

Raghuram Bathula <raghura...@gmail.com> wrote:

Be a better friend, newshound, and know-it-all with Yahoo! Mobile. Try it now.

gopal sankar

unread,
Jan 30, 2008, 9:38:44 PM1/30/08
to material...@googlegroups.com
Safety valve set pressure and system hydrotest pressure both are different concept.Safety valve set pressure is the maximum operating pressure for the particular system while in operation. Whereas the hydrotest pressure is meant to check the integrity of pipeline/vessel after fabrication/carrying modification & repair without using the process fluid. In general the safety valve set pressure is less than the system hydrotest pressure. In old practice hydrotest pressure will be 1.5 times the system design pressure and now it has been reduced to 1.3 times and IBR requirements will vary with ASME requirements.
gopalsankar
DM(INSPECTION)
Raghuram Bathula <raghura...@gmail.com> wrote:

Looking for last minute shopping deals? Find them fast with Yahoo! Search.

nachiket vagal

unread,
Jan 31, 2008, 4:54:32 AM1/31/08
to material...@googlegroups.com
I think the set pressure is 3% above the test pressure.....Shank

shailesh dave <snd...@yahoo.com> wrote:
Try it now.

Sankepalli R.S.Reddy

unread,
Feb 10, 2008, 4:38:16 AM2/10/08
to material...@googlegroups.com
As per aramco project specifications, Test RVs to be set at 5% above test pressure and tested within 1week/1month for new projects/maintenance work, respectively.
regards

srini vasan

unread,
Oct 22, 2013, 10:50:05 AM10/22/13
to material...@googlegroups.com, sankepall...@gmail.com
dear reddy
 
can i know in what std in aramco mentioned to test the RV 5% Above test pressure.
 
with regards
N.Srinivasan

Valiullah Sarpanch

unread,
Oct 22, 2013, 11:32:18 AM10/22/13
to material...@googlegroups.com

SAES-A-004

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

Ratheesh Ramachandran

unread,
Oct 22, 2013, 11:45:26 AM10/22/13
to material...@googlegroups.com
Dear Mr. Srinivasan,

you can refer to SAES A 004 for relief valve set pressure requirements

regards
Ratheesh.R
Ksa

LALU RAJENDRAN

unread,
Oct 23, 2013, 3:26:00 AM10/23/13
to material...@googlegroups.com
Dear Mr. Dave 

As per our client's requirement, we calibrate the RV at 1.1 times of the actual test pressure.

Regards 

LALU R.P

ashbandy...@gmail.com

unread,
Apr 3, 2020, 1:41:57 AM4/3/20
to Materials & Welding
Agree, for pneumatic tests the RVs are set at 110 percent of test pressure followed by reducing the pressure to 90 percent of test pressure and further reducing it to design pressure or operating pressure and go for the weld snoop test.

regards,

ashish bandyopadhyay

> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an

> For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to material...@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.

Vinay Thattey

unread,
Apr 3, 2020, 2:32:06 AM4/3/20
to material...@googlegroups.com
pressure range of RV is also important.


---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6ec8ff80-eafb-4bcc-ad4e-a04c51bacd27%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages