interruption limitations to stop welding

414 views
Skip to first unread message

sankar krishnan

unread,
Apr 1, 2021, 2:51:58 AM4/1/21
to Materials & Welding
Dear All ,

  In our Pressure vessel project 10mm thickness plate they using (GTAW+SAW) process , They have welded GTAW with 4 mm of 10mm thickness and leave open for 1 days .. I like to Know what is the interruption limitations to stop welding Limits for <19mm thickness 

Please send me code documents 

Vishwas Keskar

unread,
Apr 1, 2021, 3:59:21 AM4/1/21
to material...@googlegroups.com
what is the material being welded "
CS ,Cr Mo or SS 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0ca6ac61-bff9-444e-bc40-80249c545c8dn%40googlegroups.com.

mahesh chilukamari

unread,
Apr 1, 2021, 5:33:50 AM4/1/21
to material...@googlegroups.com
Hi,
Refer to below from ASME B31.1


--

Kannayeram Gnanapandithan

unread,
Apr 1, 2021, 7:10:03 AM4/1/21
to materials-welding
referring code
If it is ASME, no restriction
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


--

sankar bombay

unread,
Apr 1, 2021, 11:14:14 PM4/1/21
to material...@googlegroups.com
i am looking ASME VIII div1 , requirement same above as per project specification below details , I am looking for <19mm 
P1 through P5B materials with wall thickness  19 mm (0.75 in.) shall only be
interrupted provided a minimum of 10 mm (0.375 in.) of weld metal has been deposited or 25 percent of the weld
groove has been filled, whichever is greater. If welding is interrupted, the weld shall be covered with adequate
insulation to ensure slow cooling. The partially completed weld shall be 100 percent MT-inspected prior to
resuming welding.



--
shankar

George Dilintas

unread,
Apr 1, 2021, 11:14:14 PM4/1/21
to material...@googlegroups.com
Why you are trying to find problems when there is not

--

sankar bombay

unread,
Apr 1, 2021, 11:14:14 PM4/1/21
to material...@googlegroups.com
Brother 
   What about stress concentration and Oxidation of weld material , fast cooling at open atmosphere, How they will maintain the interpass temperature to avoid delay cracks 
these are the thing to be considered for low thickness , if i am wrong let me correct myself 



--
shankar

sankar bombay

unread,
Apr 1, 2021, 11:14:14 PM4/1/21
to material...@googlegroups.com

Vishwas Keskar

unread,
Apr 1, 2021, 11:38:21 PM4/1/21
to material...@googlegroups.com
10mm Carbon steel
No problem will be there. 
Just carry out Visual Inspection of the weld and proceed for subsequent Welding 

satesh kumar

unread,
Apr 2, 2021, 6:55:26 AM4/2/21
to Materials & Welding
according to you its good engineering practice?, all problem finding will give good result , all code book they finding problem and solve result at next edition  

Vinay Thattey

unread,
Apr 4, 2021, 10:36:49 PM4/4/21
to material...@googlegroups.com
Need more details . Material to be welded i.r P No etc

--

Xuân Thông

unread,
Apr 5, 2021, 4:28:56 AM4/5/21
to material...@googlegroups.com
Hi sir, 
The stop welding may be to check any cold cracking if any prior to weld the next layers

Vào Th 5, 1 thg 4, 2021 vào lúc 13:51 sankar krishnan <sankar...@gmail.com> đã viết:
Dear All ,

  In our Pressure vessel project 10mm thickness plate they using (GTAW+SAW) process , They have welded GTAW with 4 mm of 10mm thickness and leave open for 1 days .. I like to Know what is the interruption limitations to stop welding Limits for <19mm thickness 

Please send me code documents 

--