Percentage of RT As Per ASME B31.3

4,735 views
Skip to first unread message

Mukul

unread,
Apr 11, 2018, 6:53:59 AM4/11/18
to Materials & Welding
Dear Experts,

Can anybody help me by telling the RT percentage in ASME B31.3 ? Is the percentage is mentioned in the code or not ?




Regards,

Mukul Samad

George Dilintas

unread,
Apr 11, 2018, 7:03:38 AM4/11/18
to Meghanadh K
start reading 341.4
for normal fluid services, RT is 5%.
For severe cyclic conditions, it is 100%
For elevated temperature service there is a requirement for the NDE during the fabrication of the pipes in the mill. 100% RT on longitudinal or spiral welds if base metal is Pno 4 or 5

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

Lu, Feng

unread,
Apr 11, 2018, 7:30:54 AM4/11/18
to Materials & Welding

Please refer to Section 341 in B31.3.  A progressive examination is specified.  For different Service Category, the extend required is different.

 

 

Zachry Group Logo

Feng Lu, Ph.D., NDE Level III
Metallurgy and Welding Engineer

Zachry Industrial, Inc.
3600 West Sam Houston Pkwy South

Suite 200

Houston, TX 77042

l...@zachrygroup.com
Office: 713.979.2648
Cell: 512 797 5777
www.ZachryGroup.com

This e-mail may contain confidential and privileged material for the sole use of the intended recipient. Any review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient (or authorized to receive for the recipient), please contact the sender by reply e-mail and delete all copies of this message.

--
https://secure-web.cisco.com/1BZeW9grcFCKq_IdyEkQgNQqqvfr8GEzZVFhoyMxRxFsD4rI5fEtjeC7sBBIKaqB4jqFNx9hQ7Nd8hL8cGzwjfHdgDgkTddGYgCpo6o7VRha-34OBwhjKMA5QlCIlAf9EZR3WvOhhIeZwGrnw71F4Jauc9DnRm77nUryRP33FO1HSBhhmBZ-lawOoxqEwA_OuywNNKPGF5OOJYHN2dwa06egph280Fe3UB-UNWnNNi7kux_g5NxPLFY0KH9LN3EONm8rRN8EZ9vG5GujY4OHcNOc6rZAX7LxV3ioVa_2JCeQk6HMPpYqODMrY-p6F8qJX_ycqiBnaSbF4XNuyDHnZtif4ZLrFckcAaWlubarKFYM/https%3A%2F%2Fmaterials-welding.blogspot.com%2F
https://secure-web.cisco.com/1Ma0WXB__-BS0ip99KF5xiBcvNikNjrBD23itdHdlU4LaF7ZSRhO_N16E_eLk3NgRLolQU1S_D1ZrSOF1XEGCECiZUwAtTCoNRO9Zsfc-0KijbIlNvop1jQd4m8-qY1WxkyVJwWtea1rRnhiYPhIrjKjYfLMsYgPprrVgMMNPViwjeey4hpDP9sdmwEr0Gq4qWhCbasrZQ7SM0ouZwhCCbBLbVMQaVmJldK67fbjZlrpx9t9-50-t4aUgVkPcjF2XJbpNxYhXzrQ6VcmNdi5cNbBAN0fYeqIExSOUyPqMV3TIfQS49J1jnjx4p6gjb1o6nEVmuyJ_n7b2ganWmrVzzgSNGcn6ZPvdkGQJc8B-wJg/https%3A%2F%2Fwww.linkedin.com%2Fgroups%2F122787


---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://secure-web.cisco.com/1IiUw1fHt9gr9IujEEZxRlfcgeltVLr_Gg6e-UsqWhjUIk6eYgK6CyJTv8-WDGxLlWca0EyO94W6Mw8sp0Bxm1gw7hA9tmTYD2u1I8EAG76D61BQ2xqLBDKnkemH0vYMC_aEzx2ymknek15OZLGeJ9uoU4I87-ia-2jufpVK-n1AKYIpoyVk9rJWLpWy5nc_xDlgXbVzKiqs5NfwtOIhrKJ4G5wCy4LV9N9ZjBGKF3f8h8h8HlToAAUbrKtHB_3l7cOXkrDPa0ePDwhL9OP4dWdvonNrmWghXlOBSIWBf5tQRTFRLGS9KUxIa35SXGlpRTO7LEsOZofCspv9hybPU22KUn2inkzPNh6pCvxZZmko/https%3A%2F%2Fgroups.google.com%2Fgroup%2Fmaterials-welding.
For more options, visit https://secure-web.cisco.com/1GlQIJO9hqjDueIUoGngnkRMYF6_bto4PIXVE2qHSbDK8V-pneNBBmPJ9xaHXv95JvZD-XZB_VQk_8Qd_dnqQlcrHnJ2ZIiHukHqkDmaR8gE58SGGsUy04RAeRBrAi2LLLMfpNI8qYyF5ZKrvQktB_QA1Iwy7KEPGzE8Imn2S0H5pKHvW8yGq9vN0_HJdsjU43AzWcIbp2dzTdJ5jTNR5rA2cLB-eR_ZhJnzyUzLtvSKvcf6ZIwXrqx4ls-tZUGSVBFaP9eJZ2Jul82Rt6KmkVj31Dk2lC2XTsS8Xk5u2Lj2OyCW02Z0z3-iD7FNCSDteMhFXD6qXajGxH9JmYBpXfm76Trijhys8vIZFvYXd2jg/https%3A%2F%2Fgroups.google.com%2Fd%2Foptout.

Perumal Govindan

unread,
Apr 11, 2018, 8:29:38 AM4/11/18
to material...@googlegroups.com

Hi Mukul,

It's a project requirement, ASME B31.3 will indicates the fluid service categories.

Percentage of radiography is normally mentioned in the NDT requirements of Client/Welding and NDT Specification.

Also, you can refer project (PMS) Piping material specification / Piping line list / Isometric Drawing.

The requirements are mentioned in the approved line list is the final and follow the same.

Thanks


---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Mukul Hossen

unread,
Apr 11, 2018, 8:49:32 AM4/11/18
to material...@googlegroups.com
Ok.I got your point. So for category M fluid service what will be the RT percentage? 

On Wed, Apr 11, 2018, 6:29 PM Perumal Govindan <perumal...@gmail.com> wrote:

Hi Mukul,

It's a project requirement, ASME B31.3 will indicates the fluid service categories.

Percentage of radiography is normally mentioned in the NDT requirements of Client/Welding and NDT Specification.

Also, you can refer project (PMS) Piping material specification / Piping line list / Isometric Drawing.

The requirements are mentioned in the approved line list is the final and follow the same.

Thanks

On Apr 11, 2018 13:53, "Mukul" <mukulh...@gmail.com> wrote:
Dear Experts,

Can anybody help me by telling the RT percentage in ASME B31.3 ? Is the percentage is mentioned in the code or not ?




Regards,

Mukul Samad

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Perumal Govindan

unread,
Apr 11, 2018, 9:49:29 AM4/11/18
to material...@googlegroups.com

We can't decide this,  Piping  Design / Process Engineering team decides the percentage requirement of RT and indicated the requirements in the piping line list.

I believe we can't simply follow ASME B31. 3.

On Apr 11, 2018 15:49, "Mukul Hossen" <mukul.h...@gmail.com> wrote:
Ok.I got your point. So for category M fluid service what will be the RT percentage? 

On Wed, Apr 11, 2018, 6:29 PM Perumal Govindan <perumal...@gmail.com> wrote:

Hi Mukul,

It's a project requirement, ASME B31.3 will indicates the fluid service categories.

Percentage of radiography is normally mentioned in the NDT requirements of Client/Welding and NDT Specification.

Also, you can refer project (PMS) Piping material specification / Piping line list / Isometric Drawing.

The requirements are mentioned in the approved line list is the final and follow the same.

Thanks

On Apr 11, 2018 13:53, "Mukul" <mukulh...@gmail.com> wrote:
Dear Experts,

Can anybody help me by telling the RT percentage in ASME B31.3 ? Is the percentage is mentioned in the code or not ?




Regards,

Mukul Samad

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

Dokebi

unread,
Aug 4, 2020, 1:10:30 PM8/4/20
to Materials & Welding
that's right. this is correct answer.

2018년 4월 11일 수요일 오전 9시 49분 29초 UTC-4, perumal govindan 님의 말:

We can't decide this,  Piping  Design / Process Engineering team decides the percentage requirement of RT and indicated the requirements in the piping line list.

I believe we can't simply follow ASME B31. 3.

On Apr 11, 2018 15:49, "Mukul Hossen" <mukul....@gmail.com> wrote:
Ok.I got your point. So for category M fluid service what will be the RT percentage? 

On Wed, Apr 11, 2018, 6:29 PM Perumal Govindan <perumal...@gmail.com> wrote:

Hi Mukul,

It's a project requirement, ASME B31.3 will indicates the fluid service categories.

Percentage of radiography is normally mentioned in the NDT requirements of Client/Welding and NDT Specification.

Also, you can refer project (PMS) Piping material specification / Piping line list / Isometric Drawing.

The requirements are mentioned in the approved line list is the final and follow the same.

Thanks

On Apr 11, 2018 13:53, "Mukul" <mukulh...@gmail.com> wrote:
Dear Experts,

Can anybody help me by telling the RT percentage in ASME B31.3 ? Is the percentage is mentioned in the code or not ?




Regards,

Mukul Samad

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.

Mr. Sabi

unread,
Aug 5, 2020, 10:53:56 PM8/5/20
to material...@googlegroups.com
It is based service and company procedure.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

atul khatri

unread,
Aug 6, 2020, 5:47:04 AM8/6/20
to material...@googlegroups.com
Minimum  NDT % is governed by applicable fluid service as per chapter VI of ASME B31.3.
Client can always ask for more stringent requirements.
I am attaching the NDT extent as per chapter VI for quick reference.

Best regards,
ATUL Khatri


On Aug 6, 2020 8:23 AM, "Mr. Sabi" <sab...@gmail.com> wrote:
It is based service and company procedure.


On Wed, Apr 11, 2018 at 2:53 PM Mukul <mukulh...@gmail.com> wrote:
Dear Experts,

Can anybody help me by telling the RT percentage in ASME B31.3 ? Is the percentage is mentioned in the code or not ?




Regards,

Mukul Samad

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHma%3D444xNCDo1M_Wh3WsAeM1ys%3DNFKBnQo%3D_yN9i-A89CquDg%40mail.gmail.com.
Extent of NDT as per ASME B31.3.pdf

José Juan Jiménez Alejandro

unread,
Aug 6, 2020, 11:12:22 PM8/6/20
to material...@googlegroups.com
The minimum% NDT is governed by the applicable fluid service per ASME B31.3 Chapter VI.
The client can also request less stringent requirements, based on their own criteria and interests, this is totally valid, in the vast majority of countries the Code does not have legal implications, these criteria can be described in contracts, I mention it, since I am in a paper mill project, where most of the pipes carry water or water with pulp and therefore the interested company only requires 20% RT in the welded joints of the pipe systems. In other words, only some parts of the Code apply, it is only a reference, it is not mandatory in all its sections or parts.

El jue., 6 ago. 2020 a las 4:47, atul khatri (<atul....@gmail.com>) escribió:
Minimum  NDT % is governed by applicable fluid service as per chapter VI of ASME B31.3.
Client can always ask for more stringent requirements.
I am attaching the NDT extent as per chapter VI for quick reference.

Best regards,
ATUL Khatri

On Aug 6, 2020 8:23 AM, "Mr. Sabi" <sab...@gmail.com> wrote:
It is based service and company procedure.


On Wed, Apr 11, 2018 at 2:53 PM Mukul <mukulh...@gmail.com> wrote:
Dear Experts,

Can anybody help me by telling the RT percentage in ASME B31.3 ? Is the percentage is mentioned in the code or not ?




Regards,

Mukul Samad

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CACKOSeCtJr%2BfATbPr4sw_F_W%2BL6d3oyGNqhj3bo%2B7ZUU4m44wg%40mail.gmail.com.


--

Ing. José Juan Jiménez Alejandro

Independent Consultant in Parts

and Pressure Equipment

SUMMIT MÉXICO - TPI

https://www.linkedin.com/in/summit-m%C3%A9xico-tpi-760047137/

Móvil +52 1 812 352 4606