Article 344.5.2 specifies 100% radiography for girth and miter groove welds in paragraph - Reference to definition of "Girth and Miter Groove welds"

1,548 views
Skip to first unread message

Oscar Artica

unread,
Jun 27, 2015, 2:38:11 AM6/27/15
to material...@googlegroups.com
Hello Experts,

Could anyone explain what the definition of "Girth and Miter" groove welds are? I can't seem to find the definition anywhere and only mentioned in this passage of B31.3. Thanks!


John Henning

unread,
Jun 27, 2015, 5:31:31 PM6/27/15
to material...@googlegroups.com

circumferential welds in pipe 

mitered welds still circumferential but cut on an angle to make a bend.




From: material...@googlegroups.com <material...@googlegroups.com> on behalf of Oscar Artica <oscar...@gmail.com>
Sent: Friday, June 26, 2015 9:11 AM
To: material...@googlegroups.com
Subject: [MW:23119] Article 344.5.2 specifies 100% radiography for girth and miter groove welds in paragraph - Reference to definition of "Girth and Miter Groove welds"
 
Hello Experts,

Could anyone explain what the definition of "Girth and Miter" groove welds are? I can't seem to find the definition anywhere and only mentioned in this passage of B31.3. Thanks!


--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/45f8412f-e4a0-4d9b-ac6d-ae3991a2bdf0%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

muhammad usman shafiq

unread,
Jun 27, 2015, 10:29:30 PM6/27/15
to material...@googlegroups.com

Miter and girth means angle in circumferencial in weld to bend the the pipe it should be less than 15 degree.

M.Usman
Welding engineer
API 577, AWS CWI, API 510
Descon Engineering Ltd