Dear Vikas,
You have ask question in very broad prespective.
Their are many reason to say RT is better that UT.
But to convice exactly opposite to your client you need to give some more details like
1.Type of material i.e pipe or plate
2.Size-Thickness,Dia.....
Above all design code
Note that if design code ask for RT then in no way u can escape from RT unless code give relaxation in case of joint whose RT is not possible due to complex joint configuration.
Regards
Sachin
![]() |
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/XfJ-uN8RiqM/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-weld...@googlegroups.com.
Dear Rana
Carefully read below mentioned details for your information.
ULTRASONIC TESTING
UT is used to locate surface and sub surface defects in many materials plastics and wood. It is also used to measure the thickness of the materials
ADVANTAGES OF UT
1. It is sensitive to both surface and sub surface discontinuities.
2. The depth of penetration for flaw detection is superior to other NDT method.
3. Only single sided access is needed when the pulse –echo technique is used.
4. It is high accuracy in determining and estimating size and shape.
5. Fast result and very sensitive to planar type discontinuity.
6. Applicable for thick materials
DISADVANTAGES OF UT
1. Surface must be accessible to transmit ultrasound
2. Skill and training is more extensive than with other methods.
3. It normally requires a coupling medium ( except LR UT) to promote transfer of sound energy into the test specimen.
4. Materials that are rough irregular in shape very small, exceptionally, thin or not homogeneous are difficult to inspect.
5. Cast iron and other course grained materials are difficult to inspect due to low sound transmission and high signal noise.
6. Linear defects oriented parallel to the sound beam may go undetected.
7. Reference standards are required for both equipment calibration and characterization of flaws.
8. Not capable of detecting defect whose plane is parallel to the direction of sound beam.
RADIOGRAPHY TESTING
The radiation used in radiography testing is a higher energy version of the electromagnetic waves .The radiation can come from an X-Ray generator or a radioactive source.
ADVANTAGES OF RT
1. Used to inspect almost any material for surface and sub surface defects.
2. It can also be used to locates and measures internal features, confirm the location of hidden parts in an assembly.
3. Ability to inspect complex shapes and multi-layered structures without disassembly.
4. Minimum part preparation is required.
5. Capable of exposing fabrication errors at different stages of fabrication
DISADVANTAGES OF RT
1. Extensive operator training and skill required.
2. Access to both sides of the structure is usually required.
3. Orientation of radiation beam to non volumetric defects is critical.
4. Higher thickness radiography can be time consuming.
5. High experience need to proper interpretation of results.
6. Time consuming for result.
7. RT film is a permanent record of testing in the form of hard report.
8. Two dimensional image of defect is much easier and clear to interpret.
9. Job temperature should not exceed 60Deg .
10. Film is very sensitive to temperature, pressure and humidity.
Regards
Madhusoodhanan Nair.G
09967901872
Sr Inspector (VCS Quality Services Pvt Ltd,Mumbai)
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2de5b950-c3ff-4b99-9dc2-b89cdde86c90%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAE12Qq7iAaokWpbMQ%2Bw7Ctni5w60EZwQbkvSVx3-H%3D1nqu_0aA%40mail.gmail.com.
In radiography there has to be a difference in the material along the path of the beam for a defect to show up. If the beam aligns with the lack of fusion then it should be apparent, but normally the beam is not aligned along the defect. For example if you are welding with a 60 degree bevel and the lack of fusion is on the bevel surface the beam, which is aligned perpendicular to the surface will see no path or density difference in the material and hence it will not be registered on the radiograph.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eN8KLCtFDRAZBp6%3DwbQXJ_5%2BR%3DOXZwG0UETYQw5cBLjag%40mail.gmail.com.