Can anyone give me code reference for J groove bevel end requirement above 22mm wall thickness. Is it mandatory to go for J groove.?
| From: Prabhakar Raj Sent: Τετάρτη, 22 Απριλίου 2015 - 06:55 To: materials-welding@googlegroups com Reply To: material...@googlegroups.com Subject: [MW:23137] J groove bevel end requirement |
Can anyone give me code reference for J groove bevel end requirement above 22mm wall thickness. Is it mandatory to go for J groove.?
Yes I agree with all of you. To reduce heat input, weld metal and avoid distortion, J or U groove is preferred.
But, our vendor does not have the facility to do U or J groove.
So, is it acceptable to use V groove above 30mm wall thickness as per international codes.
Thanks & Regards,
G.Prabhakar Raju
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/790943679.1390822.1429700156937.JavaMail.yahoo%40mail.yahoo.com.
I agree with the recommendation below but it is not always possible.
You need to consider your interpass temperature requirements, the amount of weld volume with the v joint, do you need to grind the root pass and possibly the hot pass and how you will place the stringer beads in this weld joint.
Just a few considerations.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2B-71w-QXwATtVpGbYkG6%2BcknT6MonMGSJw%3D5%3Dg8%3DWN-hgFD7g%40mail.gmail.com.
Can anyone give me code reference for J groove bevel end requirement above 22mm wall thickness. Is it mandatory to go for J groove.?
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2B-71w9oYr_5Wb2e8MxKXSn_oWGa2YDv%2BQkOheTDE-D_ZoYRgA%40mail.gmail.com.