welding of HARDOX 500 to CS Plates

78 views
Skip to first unread message

Hani Al Masry

unread,
Mar 14, 2021, 11:42:45 PM3/14/21
to material...@googlegroups.com
Dear All 

which electrode can be used for welding of HARDOX 500 to CS Plates 

Regards,
H.A 

Aditya Gujar

unread,
Mar 15, 2021, 2:17:41 AM3/15/21
to material...@googlegroups.com
Dear Sir,

As per the Hardox manufacturer recommendation, you may go for AWS E307 type of welding consumable without any preheating. 


Regards,

Aditya Gujar
Essen Welding Alloys Pvt. Ltd.,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKOkEzc0WxOA%3DF3ft98VJOenqO_X6SN0WMmJMVNeOE4Va9d0pw%40mail.gmail.com.


--
--
 
Aditya Gujar
Sales Manager
Essen Welding Alloys Pvt. Ltd.,
Pune, India.
 
Tel: 91 20 65781493
Mob: 91 9850958075
---

Rahul Rathod

unread,
Mar 15, 2021, 2:17:47 AM3/15/21
to material...@googlegroups.com
For joining or build up?

--

Hani Al Masry

unread,
Mar 15, 2021, 11:30:37 PM3/15/21
to material...@googlegroups.com
THANKS , WHAT IS THE EQUIVALENT TO USE SMAW OR FCAW? 

DO WE NEED ALSO TO DO BUILD UP (HARDFACING) FOR THE WELDING FINAL WELDING LAYERS AFTER JOINING? 

Regards,
H.A 


LALIT VADADORIYA

unread,
Mar 15, 2021, 11:36:59 PM3/15/21
to material...@googlegroups.com
Dear sir,

It depends on the plate thickness because if the thickness of hardox 500 is more in that case chemical composition changes due to hardness. (like NI for less thick ni-0.2 for high ni-1.5, mo .25 to .6, cr 1 to 1.4)
Regards

Lalit Vadadoriya



On Mon, Mar 15, 2021 at 9:12 AM Hani Al Masry <hanyo...@gmail.com> wrote:
--
Reply all
Reply to author
Forward
0 new messages