Dear All,
Post weld hydrogen bake out ( Post weld baking ) is aplicable for ASTM 335 GR. P-22 material.There is any applicable standard.
Regards
Pradip

james gerald

unread,
Jun 23, 2015, 3:30:38 AM6/23/15
to material...@googlegroups.com
Please refer API Recommended Practice 934-A regarding Post Heating or DeHydrogenation Treatment

Recommended 300degC for min 1Hour.

Copy not available with me.
 
Thanks & Regards
J.Gerald Jayakumar
0091-9344954677


From: pradip kumar Sil <prad...@gmail.com>
To: materials-welding <material...@googlegroups.com>
Sent: Tuesday, June 23, 2015 9:57 AM
Subject: [MW:23103] Post Weld Hydrogen bake out...Post weld baking -P-22

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8%3DCaX1AdqLcBxo0Ni8xeX8EnyQZ7tq8zv6eOE9Ovf7hXQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


george....@gr.bureauveritas.com

unread,
Jun 23, 2015, 5:17:24 AM6/23/15
to material...@googlegroups.com

I would suggest to read and understand the chapter 2.5.3 of National Board Inspection Code - repairs and alterations

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Inactive hide details for pradip kumar Sil ---23/06/2015 08:31:19---Dear All, Post weld hydrogen bake out ( Post weld baking ) pradip kumar Sil ---23/06/2015 08:31:19---Dear All, Post weld hydrogen bake out ( Post weld baking ) is aplicable for ASTM 335



From: pradip kumar Sil <prad...@gmail.com>
To: materials-welding <material...@googlegroups.com>
Date: 23/06/2015 08:31
Subject: [MW:23103] Post Weld Hydrogen bake out...Post weld baking -P-22

--

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to


To post to this group, send email to


To view this discussion on the web visit

pgoswami

unread,
Jun 23, 2015, 7:48:46 AM6/23/15
to material...@googlegroups.com
Hello Pradip,
 
As mentioned below by Gerald and Dr. Georgios Dilintas(in another email) , a bake out @ 250-300 Deg C for 1-2 hrs would be advisable. The variables are :-
  • section thickness(25 mm or more)
  • H4 or Non H8 category of welding consumables.
If  welding is done  by GTAW (all through) then bake out may not be required at all or could be very minimal, @ 30 mins max (for mental comfort), to satisfy all  requirements.
 
Thanks.

 
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineer/Specialist
Ontario, Canada
 


From: material...@googlegroups.com [mailto:material...@googlegroups.com]
Sent: Tuesday, June 23, 2015 2:39 AM
To: material...@googlegroups.com
Subject: Re: [MW:23104] Post Weld Hydrogen bake out...Post weld baking -P-22

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/561924799.3748955.1435041510885.JavaMail.yahoo%40mail.yahoo.com.

pradip kumar Sil

unread,
Jun 23, 2015, 1:35:09 PM6/23/15
to materials-welding
Dear Mr. Jayakumar,
Thanks for your valuable reply. For fossil power plant,there is any applicable code for particular issue.
Regards