Autogeneous x homogeneous x heterogeneous welding

4,157 views
Skip to first unread message

Anban

unread,
Sep 22, 2013, 10:28:38 PM9/22/13
to material...@googlegroups.com
 Dear Experts
 Pls define with some samples and its applicability
 Thanks
 

Saravanan Sornam

unread,
Sep 23, 2013, 3:07:37 AM9/23/13
to material...@googlegroups.com
Dear Anban ,

You can refer from the terminology section AWS A3.0 and other welding technology books for the following in more details :

1) Autogenous Weld -      A fusion weld made without filler metal.  - Examples are Solid Phase welding, resistance welding , sometimes GTAW used in tube to tubesheet in Heat Exchangers without adding Filler .
2) Homogeneous Weld -   A fusion weld made with filler , in which the filler is similar to basemetal chemical and mechanical properties . Examples, Arc welding like SMAW, GTAW, FCAW, SAW, GMAW etc.
3) Heterogeneous Weld -  A fusion weld made with filler material which is different from the parent material - Examples are Soldering and Brazing .

Hope this clarifies .

Cheers,
Saravanan ,
Korea


--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

sudhakar kuppuswamy

unread,
Sep 23, 2013, 2:07:38 AM9/23/13
to material...@googlegroups.com

Anban,

Answers are follows,

Autogenous welding:

If a weld is made without any addition of filler metal is termed as Autogeneous weld.

Thin tube to tube sheet Austenitic stainless steels can be welded using GTAW process without addition of filler metal can be called as autogenous welding.

Using Electro beam & laser, autogenous welding can also be done

Homogeneous Welding:

If a weld is made with addition of filler metal, where the composition of filler metal is equal to the composition of base metal to be welded, good example is Welding 316L Austenitic stainless steels with 316L filler metal.

 

Heterogeneous Welding:

If a weld is made with addition of over alloyed filler metal, i.e. the chemical composition of the filler metal will be superior than the base metal.Good example is welding of Duplex stainless steel base metal say 2209 UNS S31803 using super duplex stainless steel filler metal say ER 2594.

 

With regards

Sudhakar.K



--