Hello expert ,
We are having 10% RT, pipe size is 16inch, please suggest should I select one complete joint or one segment of all the joints. Please provide the codal reference if any ?

mohammed yousuf

unread,
Dec 7, 2019, 2:40:20 AM12/7/19
to material...@googlegroups.com
Dear,

how many total joint in this line class ???



On Sat, Dec 7, 2019 at 8:40 AM Aakash <haren...@gmail.com> wrote:
Hello expert ,
We are having 10% RT, pipe size is 16inch, please suggest should I select one complete joint or one segment of all the joints. Please provide the codal reference if any ?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/01379daa-22dd-4bfd-ae0b-335e77f9e8d5%40googlegroups.com.

Balajirajan Palanisamy

unread,
Dec 8, 2019, 11:10:42 PM12/8/19
to material...@googlegroups.com
Dear Akash,
   You need to select 10% of complete joint RT in total number of joints. i.e 1 joint per 10 joints.

Normal practice, If you have more than one welder, then 10% of joints you should select from the number of welds did by that welder, as that you can cover 10% RT for that line class and also for the welders. By this you can come to know the integrity of weld and also the welder performance.

On Sat, Dec 7, 2019 at 8:40 AM Aakash <haren...@gmail.com> wrote:
Hello expert ,
We are having 10% RT, pipe size is 16inch, please suggest should I select one complete joint or one segment of all the joints. Please provide the codal reference if any ?

syed moinul hasan

unread,
Dec 8, 2019, 11:10:42 PM12/8/19
to material...@googlegroups.com
Hi. Greetings
you should take full weld , not a segment to check the soundness of weld.
As far as code is concerned, code don't says about it  ;  it is depend upon the service of the line  and project Specification, which you need to comply.

Tajuddin Mohammed

unread,
Dec 10, 2019, 10:23:46 PM12/10/19
to material...@googlegroups.com
Please select one joint for RT out of 10 joints welded

We are following this practice here in saudi Aramco 


Mohammed Tajuddin

On Sat, 7 Dec 2019, 8:40 am Aakash, <haren...@gmail.com> wrote:
Hello expert ,
We are having 10% RT, pipe size is 16inch, please suggest should I select one complete joint or one segment of all the joints. Please provide the codal reference if any ?

Adam Janzeer

unread,
Dec 10, 2019, 10:23:46 PM12/10/19
to material...@googlegroups.com
Dear 
The random selection of radiography shall be equally distributed over all welders and all type of welds, which includes welding procedure, pipe size, thickness,
welding position, etc. Progressive sample examination for piping system or pipeline based on joint not segment

atul khatri

unread,
Dec 10, 2019, 10:23:51 PM12/10/19
to material...@googlegroups.com
Totally agree with Mr. Balajirajan's reply.
10% of each welder and total 10% of all the welds. If you have some welds at shop and some at field than choose field joints for radiography test.

Thanks & Regards
Atul Khatri

Jason

unread,
Dec 27, 2019, 1:15:46 AM12/27/19
to Materials & Welding
B31.3

在 2019年12月7日星期六 UTC+3上午8:40:13,Aakash写道:

harenath jha

unread,
Dec 28, 2019, 3:49:02 AM12/28/19
to material...@googlegroups.com
Please not readable

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages