IMPACT VALUE SUBSIZE

41 views
Skip to first unread message

Elavarasan Mech

unread,
May 24, 2025, 9:14:40 AM5/24/25
to material...@googlegroups.com
Dear all 
please clarify below 
We have qualified WPS base metal thickness 6 mm P1 material as per ASME SEC IX 
PQR impact test carried out on (-10DEG C )Specimen size 10x3.3x55mm 
Can we use this PQR to production weld -20deg c project please guide me 

Regards 
ELAVARASAN

haroon mohammed

unread,
May 25, 2025, 1:52:12 PM5/25/25
to material...@googlegroups.com
No, we can't use this wps for production material

Thanks & Regards
Mohammed Haroon. K

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ynNx_-57SM1YbFA_O8_9Fm1t5E5DC11t6PBXgh6%3DkB4Kw%40mail.gmail.com.

George Dilintas

unread,
May 26, 2025, 4:26:55 AM5/26/25
to material...@googlegroups.com
Only in the case when you can increase the impact test temperature using UCS -66
Δρ. Γεώργιος Διλιντάς
Ηπείρου 5 , Μελίσσια - 15127
Αεροναυπηγος Μηχανικός - Μελος ΤΕΕ 55018
Τηλ +30 210 8100578, +30 6944 646 204

Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I,  Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis


Reply all