Hai everyone 
     I want to know the pressure vessel mill tolerance (thickness) for SA 516 GR 70 N ...which ASME code mentions the tolerance ....is it acceptable to shorten
My plate thickness is -20mm - but I got thickness is 19.6,19.7?
FOLLOWING CODE: ASME SEC VIII- DIV -01

james gerald

unread,
Apr 3, 2023, 5:45:12 AM4/3/23
to material...@googlegroups.com
Refer SA-20

Thanks & Regards

J.Gerald Jayakumar




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/505e9095-f31e-4776-9680-687561892520n%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages