Max allowable machining thickness for qualifying PQR

82 views
Skip to first unread message

JITHIN GOPINATH

unread,
May 28, 2023, 10:34:36 PM5/28/23
to material...@googlegroups.com
Sir,
Can anyone advice me about the maximum allowable machining thickness for qualifying PQR.
For example I have a pipe with thickness 15.88 I want to reduce the thickness to 12.6 is that possible? If there any limitations for machining the thickness..
Please advise...

Regards
Jithin

Vishwas Keskar Welding Manager WELDING

unread,
May 29, 2023, 12:17:37 AM5/29/23
to Materials & Welding
Jithin 
Query is not clear 
Pl. spell out clearly what is the  query  including background of the PQR in detail

Thanks 
Vishwas - IWE 

xuanth...@gmail.com

unread,
May 30, 2023, 5:02:17 AM5/30/23
to material...@googlegroups.com

No problem sir, the range qualify will be base on the actual thickness of test coupon/

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAT3KQ7iuBvsLQTWYfFSvHRunVEd%2B_jHsd_vEZMVKozOt%2BKcfw%40mail.gmail.com.


Virus-free.www.avast.com

biennd

unread,
May 31, 2023, 5:17:32 AM5/31/23
to Materials & Welding
Taping to matching thickness --> ok.

Baqer Shabbeer

unread,
May 31, 2023, 5:42:59 AM5/31/23
to material...@googlegroups.com

if you specify the design code, it will be easier to respond to your inquiry. However, according to ASME B31.3 you can Taper the wall thickness maximum to 30 degree.

--

https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

image001.jpg

paresh patel

unread,
May 31, 2023, 10:59:05 PM5/31/23
to material...@googlegroups.com
You can do machining as per your requirement But for qualification range your governing thickness will be 12.6mm. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Reply all
Reply to author
Forward
0 new messages