For pressure vessel as per asme sec 8 div 1
Client specification is asking for HIC test on PQR as per NACE TM 0284 using test solution A.
How ever acceptance criteria not specified 

Kindly advice which acceptance criteria is apicable in this case

Mhaskar Aly

unread,
Dec 13, 2021, 10:20:26 PM12/13/21
to material...@googlegroups.com
Client specs should give acceptance Criteria for HIC test

Mhaskar Ali 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOdsS42zr4Vi9as6srtbePAV0Vt7N-u7rKyt97wqcP1of8VoEg%40mail.gmail.com.

james gerald

unread,
Dec 13, 2021, 10:20:31 PM12/13/21
to material...@googlegroups.com
I suppose follow ISO 15156-2 Table B3 as below.

Inline image


Thanks & Regards

J.Gerald Jayakumar




--

Perumal Govindan

unread,
Dec 13, 2021, 10:21:15 PM12/13/21
to material...@googlegroups.com
After the test, the test specimens are cut into sections and examined under a microscope for Hydrogen Induced cracks.

 The acceptance criteria is there shall.not be a cracks.

If any cracks are found, crack length ratio, crack thickness ratio and crack sensitivity ratio will.be calculated as per NACE TM0284. 
You may enquire more information from.your local testing laboratory.

--