RE: Automatic welding machines for Pipeline Welding,

112 views
Skip to first unread message

pgos...@rogers.com

unread,
May 30, 2021, 12:11:57 PM5/30/21
to Lakshmanan Suresh Kumar, material...@googlegroups.com

Hi,

Did you look at this manufacturer’s website? Some information is as attached. There may be other manufacturer’s also, which may be available through web search.

 

Thanks.

 

Pradip Goswami.P.Eng, IWE.

Independent Consulting Welding & Metallurgical Engineering  Specialist

Saudi Aramco Approved Designated Project  Welding Engineer(DPWR)

Qatar Petroleum Approved, SME-Materials & Corrosion Engineering.

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgos...@rogers.com,pradip....@gmail.com

Cell/Whasapp:1-905-9793232

 

 

Welding Machines | crc-evans.com

 

From: Lakshmanan Suresh Kumar <sures...@gmail.com>
Sent: May 30, 2021 1:25 AM
To: material...@googlegroups.com
Subject: Automatic welding machines for Pipeline Welding

 

Gentlemen,

 

Can anyone suggest a suitable best quality automated / orbital welding machine for welding Pipeline girth Welds.

Requirements are.....

* Carbon Steel, Sour Service

* both offshore and onshore works

* open root with STT/CMT preferred

 

Thankyou

 

Regards

Suresh 

 

 

 

 

 

 


Virus-free. www.avg.com
IWM_Brochure_v04.pdf

TDK YOKESH

unread,
Jun 24, 2021, 2:55:54 AM6/24/21
to material...@googlegroups.com, Lakshmanan Suresh Kumar
Hi Lakshmanan,

QaPQA (PWT) deals with automatic Pipeline welding. We had a project done using their welding system with pipelines of size 6" to 20" which are of watll thickness 10.49mm to 50.2mm.  Kindly search for "QAPQA" in google. 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.