Please kindly advise me whether a requalification of PQR is required when changing from ER-70S2 TO ER-70S6.

Since I have a WPS qualified with ER-70S2+E7018. However, due to the non-availability of ER-70S2 can I use ER-70S6 without qualifying for new PQR.


mahesh chilukamari

ongelezen,
28 dec 2021, 22:35:3028-12-2021
aan Materials & Welding
Hi,
its a change of classification which is a supplementary essential variables , you can use the filler as proposed and it doesn't require to requalify the PQR if there is no impact test requirements.

Vishwas Keskar

ongelezen,
29 dec 2021, 01:29:4829-12-2021
aan material...@googlegroups.com
No issue.
Ensure that Mn content is less than 1.6 % before purchasing.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4de450b4-dab0-46b6-bb58-2d0aad16243fn%40googlegroups.com.
Allen beantwoorden
Auteur beantwoorden
Doorsturen
0 nieuwe berichten