Sent with Mailsuite · Unsubscribe |
06/05/24, 12:42:33 PM |
Dear Mashood,
When welding stainless steel to carbon steel or when dealing with different grades of stainless steel, the choice of filler material is critical to ensure the integrity and performance of the weld.
Using SS309 as a filler for welding SS316 to CS:
Using SS309 for welding SS316 completely:
In summary, SS309 is a suitable filler material for welding SS316 to a CS flange and is generally compatible with SS316 for welding purposes, though attention should be given to the specific application requirements.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAD3cn5hS2LbPHDo%3DciN_dsPUK9X-97b33KRO80PYso_cLw6rjw%40mail.gmail.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAADcG1qYb5mByUO-SoFmpX8zu-J1VnLGDWnuUtByt2oUdyp-6A%40mail.gmail.com.
--
--