HDPE Piping

64 views
Skip to first unread message

Anand Elankumaran

unread,
Nov 12, 2022, 8:08:31 AM11/12/22
to Materials & Welding
Dear Experts,

Could you please provide the standards for HDPE piping materials , Valves and flanges.

As far as I know, only ISO 4427-2 for pipes.

Could you please provide the remaining standards.


--
Thanks and Regards,
E. Anand,
Lead QA-QC,
Sohar,
Oman.

Perumal Govindan

unread,
Nov 12, 2022, 11:35:30 PM11/12/22
to material...@googlegroups.com
Hi
Every manufacturer has also their own manufacturer standards and most of the Client accepts based on their proven track records.

Regards 
Govindan Perumal 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANOYChzsdiw6UOn2AEtLji5La_-nUBdJ7JXwTNnpM1zUu7dUGw%40mail.gmail.com.

Hisham Mohamed

unread,
Nov 12, 2022, 11:35:39 PM11/12/22
to material...@googlegroups.com
Hi,
 Ot depends on your requirement and projects specs.
You may use: 

1. ASTM D3261
Or
2. AWWA as following (most used)

AWWA C 901-02, Standard for PE Pressure Pipe and Tubing, [13 through 76 mm] 0.5 in. through 3 in. for Water Service;
AWWA C 906-99, Standard for PE Pressure Pipe and Fittings, [102 through 1600 mm] 4-in. through 63 in. for Water Distribution and Transmission;

--

Raghuram Bathula

unread,
Nov 12, 2022, 11:42:50 PM11/12/22
to material...@googlegroups.com
EN 12201-3 for fittings
attached TWI presentation gives some insights on HDPE standards, its older one but gives lot of referances

Available Standards for Plastic presentation by TWI 21.10.2010.pdf

Kesavamoorthi Rajendiran

unread,
Nov 13, 2022, 10:21:10 PM11/13/22
to material...@googlegroups.com
ASTM D2239 --- Standard Specification for Polyethylene (PE) Plastic Pipe (SIDR-PR) Based on Controlled Inside Diameter.


ASTM D2513 --- Standard Specification for Polyethylene (PE) Gas Pressure Pipe, Tubing, and Fittings.


ASTM D2683 --- "Standard Specification for Socket-Type Polyethylene Fittings for Outside Diameter-Controlled Polyethylene Pipe and Tubing"


ASTM D2737--- "Standard Specification for Polyethylene Plastic Tubing"

ASTM D3035 --- "Standard Specification for Polyethylene (PE) Plastic Pipe (DR-PR) Based on Controlled Outside Diameter"

ASTM D3261 --- "Standard Specification for Butt Heat Fusion Polyethylene (PE) Plastic Fittings for Polyethylene (PE) Plastic Pipe and Tubing"

ASTM D3350 --- "Standard Specification for Polyethylene Plastics Pipe and Fittings Materials"

ASTM F714 ---"Standard Specification for Polyethylene (PE) Plastic Pipe (DR-PR) Based on Outside Diameter"

ASTM F1055 --- "Standard Specification for Electrofusion Type Polyethylene Fittings for Outside Diameter Controlled Polyethylene and Crosslinked Polyethylene (PEX) Pipe and Tubing"

AWWA C901-17 --- Polyethylene (PE) Pressure Pipe and Tubing, 3/4 In. (19 mm) Through 3 In. (76 mm), for Water Service

CSA B137.1 --- Polyethylene (PE) Pipe, Tubing, and Fittings for Cold-water Pressure Services




NSF International Standard 358-1 -' "Polyethylene (HDPE) Pipe and Fittings for Water-Based Ground-Source "Geothermal" Heat Pump Systems"