Difficulty in interpretation of ASME sec IX QW403.9

2,316 views
Skip to first unread message

Maulik Dodiya

unread,
Apr 18, 2013, 3:03:33 AM4/18/13
to material...@googlegroups.com
Dear Sirs,
 
I am not getting what exactly ASME Sec IX QW403.9 suggests. Can anybody help me understanding this cluase more deeply.
 
Regards,
Maulik

james gerald

unread,
Apr 18, 2013, 3:57:39 AM4/18/13
to material...@googlegroups.com
QW 403.9 states that if any weld pass in Single or Multi pass weld exceeds 13 mm (height of each individual pass) then the Base metal thickness beyond  1.1 times the Qualification thickness is an essentail variable that is for any change in Qualification Thickness beyond 1.1 T you need to qualify a new procedure.
 
Normally in SMAW,GTAW, GMAW,FCAW and mostly SAW you don't exceed 13mm of the weld metal thickness for each pass but mostly in Electrogas and Electroslag welding the Thickness exceeds 13 mm.
 
Thanks & Regards

J.Gerald Jayakumar
00968-99438165
From: Maulik Dodiya <maulik...@gmail.com>
To: material...@googlegroups.com
Sent: Thursday, April 18, 2013 11:03 AM
Subject: [MW:17461] Difficulty in interpretation of ASME sec IX QW403.9

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 


mkarya...@gmail.com

unread,
Apr 18, 2013, 7:19:26 AM4/18/13
to material...@googlegroups.com
This clauses says each pass thickness for smaw saw proces must not be more than 13mm,if it is more than 13 mm than the qualification range will be 1.1 times of PQR test plate.
-----Original Message-----
From: james gerald
Sent: 18.04.2013, 1:27 PM
To: "material...@googlegroups.com"
Subject: Re: [MW:17464] Difficulty in interpretation of ASME sec IX QW403.9


QW 403.9 states that if any weld pass in Single or Multi pass weld exceeds 13 mm (height of each individual pass) then the Base metal thickness beyond 1.1 times the Qualification thickness is an essentail variable that is for any change in Qualification Thickness beyond 1.1 T you need to qualify a new procedure.

Normally in SMAW,GTAW, GMAW,FCAW and mostly SAW you don't exceed 13mm of the weld metal thickness for each pass but mostly in Electrogas and Electroslag welding the Thickness exceeds 13 mm.

Thanks & Regards


J.Gerald Jayakumar
00968-99438165


________________________________

Chauhan Hemal

unread,
Apr 18, 2013, 8:40:03 AM4/18/13
to material...@googlegroups.com
Dear Maulik,

      This clause says if any pass in any type of welding process if more than 13 mm,the quilification thickness reange will the 1.1 times basemetal thickness.means if you found any pass more than 13 mm thickness,you can deposite weldmetal limited upto basemetal thickness used in PQR.
     Means you need to quilify WPS particularly as per job thickness wise....if your PQR test plate thickness is 30 mm you can deposite weldmetal upto 30mm only and WPS will be quilified upto that particular thickness only....and you need to quilify WPS as per job thicknesswise as per requirement....

Regards,
hemal chauhan
Engineers india limited


From: "mkarya...@gmail.com" <mkarya...@gmail.com>
To: material...@googlegroups.com
Sent: Thursday, 18 April 2013 4:49 PM
Subject: RE: [MW:17465] Difficulty in interpretation of ASME sec IX QW403.9

This clauses says each pass thickness for smaw saw proces must not be more than 13mm,if it is more than 13 mm than the qualification range will be 1.1 times of PQR test plate.
-----Original Message-----
From: james gerald
Sent:  18.04.2013, 1:27  PM
To: "material...@googlegroups.com"
Subject: Re: [MW:17464] Difficulty in interpretation of ASME sec IX QW403.9


QW 403.9 states that if any weld pass in Single or Multi pass weld exceeds 13 mm (height of each individual pass) then the Base metal thickness beyond  1.1 times the Qualification thickness is an essentail variable that is for any change in Qualification Thickness beyond 1.1 T you need to qualify a new procedure.

Normally in SMAW,GTAW, GMAW,FCAW and mostly SAW you don't exceed 13mm of the weld metal thickness for each pass but mostly in Electrogas and Electroslag welding the Thickness exceeds 13 mm.

Thanks & Regards


J.Gerald Jayakumar
00968-99438165


________________________________
From: Maulik Dodiya <maulik...@gmail.com>
To: material...@googlegroups.com
Sent: Thursday, April 18, 2013 11:03 AM
Subject: [MW:17461] Difficulty in interpretation of ASME sec IX QW403.9
 


Dear Sirs,

I am not getting what exactly ASME Sec IX QW403.9 suggests. Can anybody help me understanding this cluase more deeply.

Regards,
Maulik
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsub...@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsub...@googlegroups.com.

For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsub...@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsub...@googlegroups.com.

For more options, visit https://groups.google.com/groups/opt_out.



--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsub...@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsub...@googlegroups.com.

Binoy Soman

unread,
Apr 18, 2013, 8:17:57 AM4/18/13
to material...@googlegroups.com

Dear Maulik,

S.Binoy

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Maulik Dodiya
Sent: Thursday, April 18, 2013 10:04 AM
To: material...@googlegroups.com
Subject: [MW:17461] Difficulty in interpretation of ASME sec IX QW403.9

 

Dear Sirs,

 

I am not getting what exactly ASME Sec IX QW403.9 suggests. Can anybody help me understanding this cluase more deeply.

 

Regards,

Maulik

--
To post to this group, send email to material...@googlegroups.com

To unsubscribe from this group, send email to materials-weld...@googlegroups.com


For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Souravbohray

unread,
Sep 23, 2018, 3:52:52 AM9/23/18
to Materials & Welding
If it is greater than 13mm than impact test is complusory

Souravbohray

unread,
Sep 23, 2018, 3:52:52 AM9/23/18
to Materials & Welding
It is max or minimum generally upto 2T is max in this case instead of 2T ,1.1T than what is minimum thickness

Mohamed Elsayed

unread,
Mar 28, 2020, 3:02:03 AM3/28/20
to Materials & Welding
Thank you for the informative response. 


On Thursday, 18 April 2013 02:57:39 UTC-5, gerr...@yahoo.com wrote:
QW 403.9 states that if any weld pass in Single or Multi pass weld exceeds 13 mm (height of each individual pass) then the Base metal thickness beyond  1.1 times the Qualification thickness is an essentail variable that is for any change in Qualification Thickness beyond 1.1 T you need to qualify a new procedure.
 
Normally in SMAW,GTAW, GMAW,FCAW and mostly SAW you don't exceed 13mm of the weld metal thickness for each pass but mostly in Electrogas and Electroslag welding the Thickness exceeds 13 mm.
 
Thanks & Regards

J.Gerald Jayakumar
00968-99438165
From: Maulik Dodiya <maulik...@gmail.com>
To: material...@googlegroups.com
Sent: Thursday, April 18, 2013 11:03 AM
Subject: [MW:17461] Difficulty in interpretation of ASME sec IX QW403.9
Dear Sirs,
 
I am not getting what exactly ASME Sec IX QW403.9 suggests. Can anybody help me understanding this cluase more deeply.
 
Regards,
Maulik
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to material...@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.

George Dilintas

unread,
Mar 30, 2020, 1:15:23 AM3/30/20
to material...@googlegroups.com
This is an essential variable and must be addressed in WPS of the following processes:
SMAW
SAW
GMAW & FCAW
ESW
EGW
a YES or NO has to be entered in the WPS if any of the above processed is involved. 


---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4114043c-9707-4775-a2d3-28bf80b7d8dd%40googlegroups.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
Reply all