Request your kind expert advice on below query.

 

Vessel have Nozzle with Insert plate. External pressure stiffener ring is passing over Insert plate. Is this allowed as per code? Can we notch the stiffener ring to suit the insert plate shape outside vessel? Shift of Stiffener ring is not possible to no space available..

 

Request your prompt positive advise.

 

Thanks and best regards

 

Joshi

 




***DISCLAIMER NOTICE: ***

"The information contained in this email and/or any attachment hereto is strictly confidential and privileged. If you are not the intended recipient, and/or have received this email in error, you must not copy, disseminate or disclose the contents of this message and/or any attachment to any other person. Please notify the sender and delete this message and any attachment from your system. KNM accepts no liability in respect of prohibited and unauthorised use by an unintended addressee or recipient. Any personal views or opinions expressed by the sender shall be understood as neither given nor endorsed by KNM or any of the companies within the Group. Although this email and/or any attachment is believed to be free of any virus or other defect which may affect any computer system into which it is received and opened, it is the responsibility of the recipient to ensure that it is virus-free and KNM accepts no responsibility for any loss or damage arising in any way from the use thereof."




Rajagopal Kannan

unread,
Aug 9, 2011, 3:44:27 AM8/9/11
to material...@googlegroups.com
Dear Joshi,
First you have to Radiograph the area at which the stiffener ring passes. On satisfactory review, you can weld the Stiffener ring crossing the insert plate.
Thanks and Best Regards,
K.Rajagopal

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

murugesan jeyaraman

unread,
Aug 9, 2011, 10:04:58 AM8/9/11
to material...@googlegroups.com
Hi
 
I understand that nozzle with insert plate means as per Fig UW-14 f1 through UW-14 f4,
 
If stiffening ring overlaps the insert plate (integrally reinforced  Nozzle), it should not be a problem as you can directly weld over the insert plate.
 
If welds overlap the welding of insert plate with shell, you have to flush grind the portion of the  weld, then shoot RT and then weld the stiffening ring, do some surface NDT after welding the stiffer ring.
 
Murugesan

Rajagopal Kannan

unread,
Aug 9, 2011, 1:06:15 PM8/9/11
to material...@googlegroups.com
Dear joshi,
To be little more clear,
First you have to Radiograph the insert plate to shell weld at the location where the stiffener ring comes over the weld. On satisfactory review, you can weld the Stiffener ring crossing the insert plate to shell weld by flush grinding that particular portion.

Mohan

unread,
Feb 21, 2013, 6:59:20 AM2/21/13
to material...@googlegroups.com, material...@googlegroups.com
Hi,

I have searched for Fig UW-14 f1 through Fig UW-14 f4 in Div 1 but I couldn't find it. Please advise.

Thanks & regards
Mohan
Reply all
Reply to author
Forward
0 new messages