Dear Mr.Linoy Joseph,
As per your attached MTC in remarks, NACE MR0175/ISO 1515-2 Hardness value is HB200 MAX, wrong ISO code. If may be use, NACE MR0103 stencil mark should be in the pipe.
Please refer as below mention ISO standard,
Qualification of carbon and low-alloy steels for H2S service by laboratory testing for sour service Annex B ISO 15156-2.
Laboratory Testing of Metals for Resistance to Sulfide Stress Cracking and Stress Corrosion Cracking in H2S Environments ANSI/NACE TM0177.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/451596d7-c341-4606-9f12-78b400d16dben%40googlegroups.com.
Regards,
Tamil Neethi Thennavan
Welding Engineer
Samsung Engineering Co., Ltd
ADNOC Refining WHRB Project UAE.