PPM to mg/m2 conversion

4,803 views
Skip to first unread message

Muhammed Ibrahim PK

unread,
Mar 27, 2022, 11:14:55 PM3/27/22
to material...@googlegroups.com
Gents,

Is there any conversion available for ppm to mg/m2?

For Aramco projects, the chloride content measured in ppm using bresle patch kit in ppm.

As per Aramco spec the acceptable range is 20mg/m2.

Couldn't find the conversion. If anybody can advice, it will ne highly appreciated

Reg,
Ibrahim

james gerald

unread,
Mar 28, 2022, 2:36:28 AM3/28/22
to material...@googlegroups.com
Please correct it as 2000ppm

Thanks & Regards

J.Gerald Jayakumar




On Monday, 28 March, 2022, 09:55:17 am GMT+4, james gerald <gerr...@yahoo.com> wrote:


1% is 10000 ppm and it must be 20ppm, please check

Thanks & Regards

J.Gerald Jayakumar



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALOPgmNqFyBdfAsrXAfykfbe4-Yw%2B0hZHYxmrDWA8uHC5WUiow%40mail.gmail.com.

james gerald

unread,
Mar 28, 2022, 2:36:33 AM3/28/22
to material...@googlegroups.com
1% is 10000 ppm and it must be 20ppm, please check

Thanks & Regards

J.Gerald Jayakumar



On Monday, 28 March, 2022, 07:14:50 am GMT+4, Muhammed Ibrahim PK <ibra...@gmail.com> wrote:


--

Muhammed Ibrahim PK

unread,
Mar 29, 2022, 3:47:33 AM3/29/22
to material...@googlegroups.com
1ppm how much mg/m2?.
Is there any conversion formulae?

Reg,
Ibrahim

abdul samadh

unread,
Jul 5, 2025, 4:36:36 AM7/5/25
to Materials & Welding
 3000ppm =   50μg/cm²
(As per Elcometer kit 130 datasheet. Ref:- https://www.elcometer.com/en/elcometer-130-salt-contamination-meter.html)

μg/cm² = 10mg/m² 