[MW:5037] Pipe or Plate PQR ?

2,825 views
Skip to first unread message

Rayan Mavad Jonoob Co.

unread,
May 3, 2010, 11:33:25 PM5/3/10
to Materials & Welding
Hi dear all
Please somebody tell me if I can use a plate PQR for qualification a
pipe WPS according to ASME Sec. IX?
I could not find any thing about that in ASME code. If it's possible
then why there is pipe diameter limit in PQRs?
Please refer to ASME paragraph.

Thanks

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

BHARAT GOLE

unread,
May 4, 2010, 12:08:30 AM5/4/10
to Material Welding
Yes you can use plate PQR for qualification a pipe WPS as per ASME sect IX provided applicable P number, Group number is within limit.
As per QW 451 table no restriction for pipe diameter
 However there is restriction for pipe diameter PQR for certain consrtuction code i.e  API 1104

Bharat B. Gole

 





> Date: Mon, 3 May 2010 20:33:25 -0700
> Subject: [MW:5037] Pipe or Plate PQR ?
> From: rmj...@gmail.com
> To: material...@googlegroups.com

Catch the changing security environment Get it now.

Karthik

unread,
May 4, 2010, 12:28:45 AM5/4/10
to material...@googlegroups.com
Hi,
PQR you can use either plate or pipe..it doesn't matter...pls.rfer to QW-451 for PQR qualification limits...PQR is for P number,Welding Process,thickness .filler metal ,process...etc...its better to do the PQR with Plate for easy for welders and Procedure qualifications...Pipe diameter limits mentioned in the Section-IX only for welder's qualifications.You can use the PQR with Plate for Pipe also..When you qualify the welders for pipe  you can use the same PQR of plate with the Thickness limits and all other essential variables mentioned in QW-250 to QW-265 according to the process you are using for PQR.
If u have any doubts feel free to ask..
 
Thanks & Regards,
 
(Karthik)

Karthikeyan.S
 
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Tue, 5/4/10, Rayan Mavad Jonoob Co. <rmj...@gmail.com> wrote:

From: Rayan Mavad Jonoob Co. <rmj...@gmail.com>
Subject: [MW:5037] Pipe or Plate PQR ?

Prabhu Kumar L

unread,
May 4, 2010, 12:18:57 AM5/4/10
to material...@googlegroups.com

Dear Rayan,

 

Please refer to clause no. QW-211 of ASME Sec. IX. Also note that pipe diameter is not essential variable for PQR qualifications as per Sec. IX. However, it is essential variable for Welder performance qualifications.

 

For API 1104, pipe diameter is essential variable for PQR and welder performance qualification as well.

 

Regards,

 

L. Prabhu kumar,

Sr. Principal Engineer,

 

Equipments & Materials Dept.,

Saipem India Projects Limited,

Nungambakkam High Road, Chennai - 600 034, India.

Tel:+91 44 43906588, Ext.: 588, Fax:+91 44 66840345,

Mobile Ph. No.: +91 9003010978.





-------------------------------------------------------------------------------------------------------------------------------------------------------------------
DISCLAIMER: The information contained in this communication is intended solely for the use of the individual or 
entity to whom it is addressed and others authorized to receive it. It may contain confidential or legally privileged 
information. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution 
or taking any action in reliance on the contents of this information is strictly prohibited and may be unlawful. If 
you have received this communication in error, please notify us immediately by responding to this email and then 
delete it from your system. Saipem India Projects Limited (SIPL) is neither liable for the proper and complete 
transmission of the information contained in this communication nor for any delay in its receipt. 
-------------------------------------------------------------------------------------------------------------------------------------------------------------------

arijoy roy

unread,
May 4, 2010, 1:57:30 AM5/4/10
to material...@googlegroups.com
Dear
I have one observation. The position of welding is also important. If it is a 5 g position actual welding , will you be able to use plate for process qualification.
With Regards
Arijoy Roy
--- On Tue, 4/5/10, Karthik <karth...@yahoo.com> wrote:

Karthik

unread,
May 4, 2010, 2:17:16 AM5/4/10
to material...@googlegroups.com
hi,
PQR is not concerned with welding position.You have to qualify the welders according to The actual welding position with the applicable WPS and PQR.
 
Thanks & Regards,
 
(Karthik)

Karthikeyan.S
 
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Tue, 5/4/10, arijoy roy <bha...@yahoo.com> wrote:

Muhammed Ibrahim

unread,
May 4, 2010, 3:45:52 AM5/4/10
to material...@googlegroups.com
Hi,
 
Please note that PQR is mainly intented for proving the mechanial poperty of weld. Position is not the matter in case of ASME Sec IX if impact test requirement is not applicable.
 
In case of impact test  requiement, if you qaulify the PQR in 3G position (highest heat input position) it will qualify all position.
 
If your production weld is in 5G position you have to qualify the welder in 5G or 6G position to prove the skill of welder.
 
If the qualifiation is for pipe line as per API 1104, dia, thikness and position is matter.
 
Regards,
Muhammed Ibahim PK
--
Thanks & Regards
Muhammed Ibrahim PK

Sakib

unread,
May 4, 2010, 5:34:51 AM5/4/10
to material...@googlegroups.com

in case of impact test  requiement, if you qaulify the PQR in 3G position (highest heat input position) it will qualify all position.
 

would you please quote its reference mr ibrahim
--
with Regards


SAQIB JALAL
Inspection Engineer
PakArab Fertilizer Limited
Khanewal Road , Multan
office number +92-61-9061 EXT 3110
mobile number +92-321-4043556

kannayeram gnanapandithan

unread,
May 8, 2010, 11:32:50 AM5/8/10
to material...@googlegroups.com
No restriction for WPS, but  for welder  performance qualification there is a restriction in minimum dia say 73mm od
kgp