Hi,S275JR is unlisted material in AWS D1.1, so you have to make a new WPS.Regards,
Harish Kumar
On Sat, 18 Apr 2020, 17:02 chris, <chris...@gmail.com> wrote:
hello friends,--I have a WPS with ref code AWS D 1.1 for A36 can I use the same for welding S275JR as well?I would like to know if there is any code prohibition for this? Even though the materials are almost the same except for a higher yield strength for S275.Best regardsChris
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/86dad886-50a4-484f-a072-384c98b711c1%40googlegroups.com.