INCONEL 825

131 views
Skip to first unread message

Elavarasan Mech

unread,
May 7, 2025, 7:34:56 AM5/7/25
to material...@googlegroups.com
Dear all 
INCONEL 825 matching filler  
ER NI FECR-1 its correct please guide me

Regarding 
Elavarasan



Surendar Gunasekaran

unread,
May 14, 2025, 2:53:24 AM5/14/25
to material...@googlegroups.com
image.png

As per API RP 582, Recommended filler for Inconel 825 is E/ERNiCrMo-3

Regards,
Surendar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ynC1wRkBFZy4DdWohSf9QUxF1deT7NTk7s8mq3RXN3-_w%40mail.gmail.com.


--
With Regards
Surendar Gunasekaran

Kannayeram Gnanapandithan

unread,
May 14, 2025, 9:32:28 AM5/14/25
to materials-welding
Yes. Availability is question mark. And too much fissures. 

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015, ISO 3834, EN 15085, 
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

Parminder Singh

unread,
May 15, 2025, 12:13:38 AM5/15/25
to material...@googlegroups.com
its correct
but welding of Inconel 825 is crack prone. 
1. Use TIG welding as preferred method
2. Do qualify the PQR for proper technique establishment